Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 1.00e+11 - 1.00e+12 ohm-cm | 1.00e+11 - 1.00e+12 ohm-cm | ASTM D257 |
PolyOne Stat-Tech™ AS-1000 AS Acrylonitrile Butadiene Styrene (ABS) Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound.. |
|||
Volume Resistivity | 1.00e+10 - 1.00e+12 ohm-cm | 1.00e+10 - 1.00e+12 ohm-cm | ASTM D257 |
PolyOne Stat-Tech™ PI-05CF/000R Black Polyether Imide (PEI) Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound.. |
|||
Volume Resistivity | 1.00e+11 - 1.00e+12 ohm-cm | 1.00e+11 - 1.00e+12 ohm-cm | IEC 60093 |
Raschig Group AMPLA® 7250 melamine-modified polyester Cellulose reinforced melamine-modified Polyester molding compound. Very good electrical values, excellent heat resistance, excellent surface quality, low post shrinkage. This product meets the allow.. |
|||
Volume Resistivity | 1.00e+11 - 1.00e+12 ohm-cm | 1.00e+11 - 1.00e+12 ohm-cm | IEC 60093 |
Raschig Group AMPLA® 7500 melamine-modified polyester Organically and inorganically filled melamine modified Polyester molding compound. Low post-shrinkage, very good electrical values, excellent heat resistance, very good sliding behavior and wear sta.. |
|||
Volume Resistivity | 1.00e+11 - 1.00e+12 ohm-cm | 1.00e+11 - 1.00e+12 ohm-cm | IEC 60093 |
Raschig Group MELOPAS® 156 MF Melamine Glass fiber reinforced Melamine molding compound. This product meets the allowed upper limits for heavy metals and PCAs and also conforms to the requirements of the EU directives 2002/95 (RoHS), 200.. |
|||
Volume Resistivity | 1.00e+11 - 1.00e+12 ohm-cm | 1.00e+11 - 1.00e+12 ohm-cm | IEC 60093 |
Raschig Group MELOPAS® 2010 MF Melamine Organically and inorganically filled Melamine molding compound. Excellent surface hardness, good mechanical strength, good electrical properties. This product meets the allowed upper limits for heav.. |
|||
Volume Resistivity | 1.00e+11 - 1.00e+12 ohm-cm | 1.00e+11 - 1.00e+12 ohm-cm | IEC 60093 |
Raschig Group MELOPAS® 6605 MP Melamine Cellulose reinforced Melamine molding compound. Very good electrical properties, excellent surface hardness, good mechanical strength and heat resistance, good wear and UV-stability, good gliding be.. |
|||
Volume Resistivity | 1.00e+11 - 1.00e+12 ohm-cm | 1.00e+11 - 1.00e+12 ohm-cm | IEC 60093 |
Raschig Group MELOPLAS® 150 MF Wood flour-reinforced MF molding compound in dark colors. High surface hardness, high mechanical strength, good electrical properties. Self-extinguishing (V-O/1,6 according to UL 94), UL-listed. Fr.. |
|||
Volume Resistivity | 1.00e+11 - 1.00e+12 ohm-cm | 1.00e+11 - 1.00e+12 ohm-cm | IEC 60093 |
Raschig Group MELOPLAS® 152 MF Cellulose-reinforced MF molding compound in white and colored shades. Very good electrical properties, high surface hardness, good abrasion- and UV-stability, very good resistance to chemicals - al.. |
|||
Volume Resistivity | 1.00e+11 - 1.00e+12 ohm-cm | 1.00e+11 - 1.00e+12 ohm-cm | IEC 60093 |
Raschig Group MELOPLAS® 152.7 MF Cellulose-reinforced MF molding compound in white and colored shades. High surface hardness, very good UV stability, very good resistance to chemicals also to foodstuff ingredients, physiologically.. |
|||
Volume Resistivity | 1.00e+11 - 1.00e+12 ohm-cm | 1.00e+11 - 1.00e+12 ohm-cm | IEC 60093 |
Raschig Group MELOPLAS® 181 MF Cellulose-reinforced, phenol-modified MF molding compound (MPF) in white and colored shades. High surface hardness, good electrical properties, good mechanical strength, high UV and heat resistanc.. |
|||
Volume Resistivity | 1.00e+11 - 1.00e+12 ohm-cm | 1.00e+11 - 1.00e+12 ohm-cm | IEC 60093 |
Raschig Group MELOPLAS® 182 MF Wood flour-reinforced and inorganically filled, phenol-modified MF molding compound (MPF) in dark colors. Improved dimensional stability and electrical properties as compared with MP 180, high surf.. |
|||
Volume Resistivity | 1.00e+11 - 1.00e+12 ohm-cm | 1.00e+11 - 1.00e+12 ohm-cm | IEC 60093 |
Raschig Group MELOPLAS® 183 MF Cellulose-reinforced and inorganically filled, phenol-modified MF molding compound (MPF) in white and colored shades. Improved dimensional stability and electrical properties as compared with MP 18.. |
|||
Volume Resistivity | 1.00e+11 - 1.00e+12 ohm-cm | 1.00e+11 - 1.00e+12 ohm-cm | IEC 60093 |
Raschig Group MELOPLAS® 2500 MF Cellulose-reinforced MF molding compound in white and colored shades. Very good electrical properties, high surface hardness, good abrasion- and UV-stability, very good resistance to chemicals - al.. |
|||
Volume Resistivity | 1.00e+11 - 1.00e+12 ohm-cm | 1.00e+11 - 1.00e+12 ohm-cm | IEC 60093 |
Raschig Group MELOPLAS® 3025 MF Cellulose-reinforced and inorganically filled MF molding compound in white and colored shades. High surface hardness, good UV and heat stability, very good resistance to chemicals - also to foodstu.. |
|||
Volume Resistivity | 1.00e+11 - 1.00e+12 ohm-cm | 1.00e+11 - 1.00e+12 ohm-cm | IEC 60093 |
Raschig Group RALUPOL® 2200 UP Polyester Organically filled polyester molding compound. Low post-shrinkage, good electrical values and mechanical properties, high surface quality and good color stability (non-yellowing). This product meets.. |
|||
Volume Resistivity | 1.00e+10 - 1.00e+12 ohm-cm | 1.00e+10 - 1.00e+12 ohm-cm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-LOY A3000TXB ABS LNP* STAT-LOY* A3000TXB is a compound based on ABS resin. Added features of this material include: Antistatic, Transparent, Formulated with FDA Food Contact Additives and Bioassessed to ISO 10993... |
|||
Volume Resistivity | 1.00e+10 - 1.00e+12 ohm-cm | 1.00e+10 - 1.00e+12 ohm-cm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-LOY A3000TXJ ABS LNP* STAT-LOY* A3000TXJ is a product based on ABS resin. Added features of this material include: Antistatic, Transparent, Formulated with FDA Food Contact Additives. |
|||
Volume Resistivity | 1.00e+8 - 1.00e+12 ohm-cm | 1.00e+8 - 1.00e+12 ohm-cm | ASTM D257 |
Techmer ES Statiblend® 02036 Polypropylene Availability: North AmericaForms: PelletsAdditive: AntistaticFeatures: Antistatic and ConductiveInformation provided by TP Composites, Inc. |
|||
Volume Resistivity | 1.00e+8 - 1.00e+12 ohm-cm | 1.00e+8 - 1.00e+12 ohm-cm | ASTM D257 |
Techmer ES Statiblend® 02056 BKN Polypropylene Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified FillerReinforFeatures: ConductiveAppearance: BlackTPCI# 9109116Information provided by TP Composites, Inc. |
|||
Volume Resistivity | 1.00e+8 - 1.00e+12 ohm-cm | 1.00e+8 - 1.00e+12 ohm-cm | ASTM D257 |
Techmer ES Statiblend® 02056 Polypropylene Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified FillerReinforFeatures: ConductiveAppearance: BlackTPCI# 9111116Information provided by TP Composites, Inc. |
|||
Volume Resistivity | 1.00e+10 - 1.00e+12 ohm-cm | 1.00e+10 - 1.00e+12 ohm-cm | ASTM D257 |
Techmer ES Statiblend® ABS GF15 AS 15% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 15% Filler by WeightAdditive: AntistaticFeatures: AntistaticInformation provided by TP Composites, Inc. |
|||
Volume Resistivity | 1.00e+10 - 1.00e+12 ohm-cm | 1.00e+10 - 1.00e+12 ohm-cm | ASTM D257 |
Techmer ES Statiblend® ABS GF20 AS 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 20% Filler by WeightAdditive: AntistaticFeatures: AntistaticInformation provided by TP Composites, Inc. |
|||
Volume Resistivity | 1.00e+10 - 1.00e+12 ohm-cm | 1.00e+10 - 1.00e+12 ohm-cm | ASTM D257 |
Techmer ES Statiblend® PA6 GF20 AS BK 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 20% Filler by WeightAdditive: Antistatic, Heat Stabilizer and LubricantFeatures: Antistatic, Heat Stabilizer and Lubricate.. |
|||
Volume Resistivity | 1.00e+10 - 1.00e+12 ohm-cm | 1.00e+10 - 1.00e+12 ohm-cm | ASTM D257 |
Techmer ES Statiblend® PA6/6 GF20 AS BK 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 20% Filler by WeightAdditive: Lubricant, Antistatic and Heat StabilizerFeatures: Antistatic, Heat Stabilized and Lubricate.. |
|||
Volume Resistivity | 1.00e+10 - 1.00e+12 ohm-cm | 1.00e+10 - 1.00e+12 ohm-cm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-LOY KX01002 Acetal Copolymer (Europe-Africa-Middle East) LNP* Stat-Loy* KX01002 is a compound based on Acetal Copolymer resin containing Antistat. Added features include: Permanent Anti-Static. |
|||
Volume Resistivity | 1.00e+11 - 1.00e+12 ohm-cm | 1.00e+11 - 1.00e+12 ohm-cm | IS 3396-1979 |
Amity Thermosets ATI 102 Phenolic Molding Organic Filler, Injection Molded Characteristics:Electrical low loss Good mechanical strengthHigh electrical insulationGood mechanical strengthGlossy surfaceLow water absorptionColor-blackVery soft flow Applications: Electric swit.. |
|||
Volume Resistivity | 1.00e+11 - 1.00e+12 ohm-cm | 1.00e+11 - 1.00e+12 ohm-cm | IEC 60093 |
Raschig Group MELOPLAS® 180 MF Wood flour-reinforced, phenol-modified MF molding compound (MPF) in dark colors. High surface hardness, good mechanical strength and electrical properties, good heat resistance. Self-extinguishing .. |