Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 1.00e+10 - 1.00e+11 ohm-cm | 1.00e+10 - 1.00e+11 ohm-cm | |
LG Chemical LUPOY EC5000A PC/ABS Description: Injection Molding, PC/ABS, General Purpose, Anti-Static.Application: E&E (Housing)Information provided by LG Chemical |
|||
Volume Resistivity | 10000 - 1.00e+11 ohm-cm | 10000 - 1.00e+11 ohm-cm | |
Industrial Laminates/Norplex SP525M (WaveMax 5000) Glass Fabric Description: Non-woven substrate combined with high temperature, static dissipative epoxy resin. Superior machining properties. Capable of producing thin walls with high strength for finely machined.. |
|||
Volume Resistivity | 1.00e+9 - 1.00e+11 ohm-cm | 1.00e+9 - 1.00e+11 ohm-cm | ASTM D257 |
Techmer ES Electrablend® ABS CF5 5% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 5% Filler by WeightAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Volume Resistivity | 1.00e+8 - 1.00e+11 ohm-cm | 1.00e+8 - 1.00e+11 ohm-cm | ASTM D257 |
Techmer ES HiFill FR® PBT GF30 FR-S AS 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightAdditive: AntistaticFeatures: Flame Retardant, Antistatic and Non-BloomingProcessing Method: Injection.. |
|||
Volume Resistivity | 1.00e+7 - 1.00e+11 ohm-cm | 1.00e+7 - 1.00e+11 ohm-cm | ASTM D257 |
Techmer ES HiFill® PA6/6 0146 A Nylon 66 Availability: North AmericaForms: PelletsFiller/Reinforcement: Copper FillerFeatures: High Specific GravityInformation provided by TP Composites, Inc. |
|||
Volume Resistivity | 1.00e+7 - 1.00e+11 ohm-cm | 1.00e+7 - 1.00e+11 ohm-cm | ASTM D257 |
Techmer ES HiFill® PA6/6 0164 A Nylon 66 Availability: North AmericaForms: PelletsFiller/Reinforcement: Copper FillerFeatures: High Specific GravityInformation provided by TP Composites, Inc. |
|||
Volume Resistivity | 1.00e+9 - 1.00e+11 ohm-cm | 1.00e+9 - 1.00e+11 ohm-cm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-LOY 93000LTH Acrylic LNP* STAT-LOY* 93000LTH is a compound based on Acrylic resin. Added features of this material include: Antistatic, Transparent and Formulation Locked. |
|||
Volume Resistivity | 1.00e+9 - 1.00e+11 ohm-cm | 1.00e+9 - 1.00e+11 ohm-cm | ASTM D 257 |
SABIC Innovative Plastics LNP Stat-loy 9X05426C PMMA LNP* Stat-loy* 9X05426C is a compound based on PMMA resin containing Anti-Static. Added features of this material include: Antistat.This data was supplied by SABIC-IP for the Americas region. |
|||
Volume Resistivity | 1.00e+9 - 1.00e+11 ohm-cm | 1.00e+9 - 1.00e+11 ohm-cm | ASTM D 257 |
SABIC Innovative Plastics LNP Stat-loy 9X05426C PMMA (Asia Pacific) LNP* Stat-loy* 9X05426C is a compound based on PMMA resin containing Anti-Static. Added features of this material include: Antistat.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Volume Resistivity | 1.00e+10 - 1.00e+11 ohm-cm | 1.00e+10 - 1.00e+11 ohm-cm | ASTM D 257 |
SABIC Innovative Plastics LNP Stat-loy K3000 Acetal Copoly LNP* Stat-loy* K3000 is a compound based on Acetal Copolymer resin containing Anti-Static. Added features of this material include: Antistat.This data was supplied by SABIC-IP for the Americas regi.. |
|||
Volume Resistivity | 1.00e+10 - 1.00e+11 ohm-cm | 1.00e+10 - 1.00e+11 ohm-cm | ASTM D 257 |
SABIC Innovative Plastics LNP Stat-loy K3000 Acetal Copoly (Asia Pacific) LNP* Stat-loy* K3000 is a compound based on Acetal Copolymer resin containing Anti-Static. Added features of this material include: Antistat.This data was supplied by SABIC-IP for the Asia Pacific .. |
|||
Volume Resistivity | 1.00e+10 - 1.00e+11 ohm-cm | 1.00e+10 - 1.00e+11 ohm-cm | ASTM D257 |
SABIC Innovative Plastics LNP THERMOCOMP ECF62 PEI LNP* THERMOCOMP* ECF62 is a compound based on Polyetherimide resin containing 30% Glass Fiber, 10% Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Volume Resistivity | 1.00e+10 - 1.00e+11 ohm-cm | 1.00e+10 - 1.00e+11 ohm-cm | ASTM D257 |
SABIC Innovative Plastics LNP THERMOCOMP ECF62 PEI (Asia Pacific) LNP* Thermocomp* ECF62 is a compound based on Polyetherimide resin containing Glass Fiber, Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Volume Resistivity | 1.00e+8 - 1.00e+11 ohm-cm | 1.00e+8 - 1.00e+11 ohm-cm | ASTM D257 |
Techmer ES Statiblend® HIPS E Availability: North AmericaForms: PelletsAdditive: AntistaticFeatures: Antistatic and ConductiveAppearance: Natural ColorProcessing Method: ExtrusionInformation provided by TP Composites, Inc. |
|||
Volume Resistivity | 1.00e+9 - 1.00e+11 ohm-cm | 1.00e+9 - 1.00e+11 ohm-cm | ASTM D257 |
Techmer ES Statiblend® PA6 GF30 AS BK 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightAdditive: AntistaticFeatures: AntistaticAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Volume Resistivity | 1.00e+8 - 1.00e+11 ohm-cm | 1.00e+8 - 1.00e+11 ohm-cm | ASTM D257 |
Techmer ES Statiblend® PA6/6 GF10 BK 10% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 10% Filler by WeightAdditive: LubricantFeatures: Conductive and LubricatedAppearance: BlackInformation provided by TP Comp.. |
|||
Volume Resistivity | 1.00e+10 - 1.00e+11 ohm-cm | 1.00e+10 - 1.00e+11 ohm-cm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-KON EEF42 PEI (Asia Pacific) LNP STAT-KON* EEF42 is a compound based on Polyetherimide resin containing Carbon Fiber, Glass Fiber. Added features of this material include: Electrically Conductive. |
|||
Volume Resistivity | 1.00e+9 - 1.00e+11 ohm-cm | 1.00e+9 - 1.00e+11 ohm-cm | ASTM D257 |
Techmer ES HiFill® PA6 0254 B2 Barium Sulfate Filler Availability: North AmericaForms: PelletsFiller/Reinforcement: Barium SulfateFeatures: High Specific Gravity and AntistaticAdditive: AntistaticInformation provided by TP Composites, Inc. |
|||
Volume Resistivity | 1.00e+9 - 1.00e+11 ohm-cm | 1.00e+9 - 1.00e+11 ohm-cm | Dry; ASTM D257 |
Westlake Plastics Absylux® SD-A Acrylonitrile-Butadiene-Styrene (anti-static) Non-carbon filled anti-static material which has high impact strength, good tensile and flexural strength, and is easily machined. Available in natural or black, it can be easily thermoformed in th.. |
|||
Volume Resistivity | 1.00e+9 - 1.00e+11 ohm-cm | 1.00e+9 - 1.00e+11 ohm-cm | Dry; ASTM D257 |
Westlake Plastics Pomalux® SD-A Acetal Copolymer (anti-static) Non-carbon-filled, permanently static-dissipative material which is non-migratory and non-humidity dependent. With enhanced lubricity, POMALUX SD-A provides superior wear resistance and ease of mac.. |
|||
Volume Resistivity | 1.00e+9 - 1.00e+11 ohm-cm | 1.00e+9 - 1.00e+11 ohm-cm | Dry; ASTM D257 |
Westlake Plastics Propylux® SD-A Polypropylene (anti-static) Non-carbon-filled, permanently static-dissipative material, with good chemical resistance and mechanical properties. This material is light weight, weldable, easily machined and fabricated, availab.. |
|||
Volume Resistivity | 1.00e+7 - 1.00e+11 ohm-cm | 1.00e+7 - 1.00e+11 ohm-cm | Dry; ASTM D257 |
Westlake Plastics Zelux® SD-P Polycarbonate (static dissipative) Carbon powder filled with high flexural strength and good thermal stability to 270°F. Thermoformable in 0.010" to 0.060" gauges; low outgassing.Information provided by Westlake Plastics. |
|||
Volume Resistivity | 1.00e+10 - 1.00e+11 ohm-cm | 1.00e+10 - 1.00e+11 ohm-cm | IS 3396-1979 |
Amity Thermosets ATG 115 Phenolic Molding Organic Filler, Compression Molded Characteristics:Medium mechanical strength Medium electrical insulationGeneral purposeColor- Black, BrownSoft/medium flow Applications: Electrical accessories & fittings ( medium quality ) Domestic .. |
|||
Volume Resistivity | 1.00e+10 - 1.00e+11 ohm-cm | 1.00e+10 - 1.00e+11 ohm-cm | IS 3396-1979 |
Amity Thermosets ATG 116 Phenolic Molding Organic and inorganic Filler, Compression Molded Characteristics:Medium mechanical strength Medium electrical insulationGeneral purposeColor- BlackMedium flow Applications: Electrical accessories & fittings ( medium quality ) Domestic appliance ha.. |