Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 6.60e+16 ohm-cm | 6.60e+16 ohm-cm | IEC 60093 |
SABIC Innovative Plastics ULTEM 1285 PEI (Europe-Africa-Middle East) Transparent Polyetherimide blend. ECO Conforming. US FDA and EU Food Contact compliant in recognized colors. |