Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 6.4 ohm-cm | 6.4 ohm-cm | DIN IEC93 |
P & P Technology CB 50 Carbon Loaded Silicone Applications: Electrically conductive grades which when properly catalyzed can be considered for applications requiring conductivity such as EMI gaskets, conductive sheaths for ignition cable core,.. |