Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 6.00e+14 ohm-cm | 6.00e+14 ohm-cm | STN 34 6460 |
Plastcom SLOVAMID® 6 GF 65/2M PA6 reinforced with glass fiber PA 6 for injection molding, reinforced with 65% of glass fiber, for moldings used in the automotive, electrical, engineering and consumer-goods industry. Application: grips of electrotools, hobby to.. |
|||
Volume Resistivity | 6.00e+14 ohm-cm | 6.00e+14 ohm-cm | ASTM D257 |
Rogers Corporation TMM® TMM4 Ceramic Thermoset Polymer Composite TMM® Thermoset microwave materials are ceramic thermoset polymer composites designed for high plate-thru-hole reliability stripline and microstrip applications. The electrical and mechanical prope.. |
|||
Volume Resistivity | 6.00e+14 ohm-cm | 6.00e+14 ohm-cm | |
Momentive Performance Materials RTV112 One Component Acetoxy Adhesive Sealant, White RTV series one-component, ready-to-use adhesive sealants are extremely versatile. They cure to a tough, durable, resilient silicone rubber on exposure to atmospheric moisture at room temperature. .. |
|||
Volume Resistivity | 6.00e+14 ohm-cm | 6.00e+14 ohm-cm | |
Momentive Performance Materials RTV118 One Component Acetoxy Adhesive Sealant, Translucent RTV series one-component, ready-to-use adhesive sealants are extremely versatile. They cure to a tough, durable, resilient silicone rubber on exposure to atmospheric moisture at room temperature. .. |
|||
Volume Resistivity | >= 6.00e+14 ohm-cm | >= 6.00e+14 ohm-cm | ASTM D 257 |
Karina 951-35/4-IS-LMP Ivory PVC Compound Heavy metal free PVC compound with high electrical insulation resistance. Recommended for insulation of CI and CCI cables.Information provided by Karina Indústria e Comércio de Plásticos Lt.. |
|||
Volume Resistivity | 6.00e+14 ohm-cm | 6.00e+14 ohm-cm | |
Momentive Performance Materials TSE3940 Flame Retardant Adhesive Sealant, Gray TSE3940 and TSE3941 flame retardant adhesive/sealants are non-flowable, one-component RTVs that cure quickly by reacting with atmospheric moisture forming a soft elastic silicone rubber. These mater.. |
|||
Volume Resistivity | 6.00e+14 ohm-cm | 6.00e+14 ohm-cm | ASTM D257 |
Solvay Specialty Polymers Amodel® AS-4145 HS Polyphthalamide (PPA), 45% Glass Fiber (Conditioned) Amodel® AS-4145 HS polyphthalamide (PPA) is a 45% glass reinforced resin that is hot-water moldable. Key properties include high heat resistance, high strength and stiffness over a broad tempera.. |
|||
Volume Resistivity | 6.00e+14 ohm-cm | 6.00e+14 ohm-cm | IEC 60093 |
Polyplastics Duranex® 6300T Polybutylene Terephthalate (PBT), Low friction, Low wear, Mineral filled DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Volume Resistivity | 6.00e+14 ohm-cm | 6.00e+14 ohm-cm | |
Tra-Con Tra-Bond 723C01 One-Part Medical Grade Adhesive TRA-BOND 723C01 is a fast, heat curing, one component adhesive targeted at medical applications. The material complies with USP Class VI toxicity requirements and is resistant to gamma sterilization.. |
|||
Volume Resistivity | 6.00e+14 ohm-cm | 6.00e+14 ohm-cm | |
Dow Corning HV 1540/20P BASE AND CLEAR CURING AGENT 32 Shore, very low viscosity, castable hydrophobic silicone rubber with high tear strength and low temperature cure.Information provided by Dow Corning |
|||
Volume Resistivity | 6.00e+14 ohm-cm | 6.00e+14 ohm-cm | |
Dow Corning SLYGARD® 535 THIXOTROPIC DIELECTRIC GEL Information provided by Dow Corning |
|||
Volume Resistivity | 6.00e+14 ohm-cm | 6.00e+14 ohm-cm | dry; IEC 60093 |
DSM Novamid® 1010GN2-30 NAT/BK37 PA6-GF30 FR(17) 30% Glass Reinforced, Flame Retardant |
|||
Volume Resistivity | 6.00e+14 ohm-cm | 6.00e+14 ohm-cm | dry; IEC 60093 |
DSM Novamid® 1013G15 1 NA PA6-GF15 15% Glass Reinforced, Injection Molding |
|||
Volume Resistivity | 6.00e+14 ohm-cm | 6.00e+14 ohm-cm | dry; IEC 60093 |
DSM Novamid® 1013GH15 1 NA/BK37 PA6-GF15 15% Glass Reinforced, Heat Stabilized, Injection Molding |
|||
Volume Resistivity | <= 6.00e+14 ohm-cm | <= 6.00e+14 ohm-cm | |
Cytec (Conap) FR-1272 Conapoxy® Resin / Conacure® Hardener Epoxy Potting and Encapsulating Systems for Electronic ApplicationsHigh technology epoxy resin systems for potting and encapsulation, for the defense, aerospace, electronics, computer, automotive an.. |
|||
Volume Resistivity | >= 6.00e+14 ohm-cm | >= 6.00e+14 ohm-cm | ASTM D257 |
Fainplast Compounds Hax™ HFX 505/2 Crosslinkable HFFR Cable Compound Polyolefin based HFFR silane grafted compound; cross-linkable by heat and moisture and by addition of suitable catalystGrade description:• Sheathing; InsulationInformation provided by Fainplast Com.. |
|||
Volume Resistivity | 6.00e+14 ohm-cm @Temperature 20.0 °C |
6.00e+14 ohm-cm @Temperature 68.0 °F |
ASTM D257 |
Fainplast Compounds HAX HF 4221 Halogen Free PVC General purpose |
|||
Volume Resistivity | 6.00e+14 ohm-cm | 6.00e+14 ohm-cm | 50% RH; ASTM D-257 |
Axiall 13821 Wire & Cable Flexible PVC Non-lead stabilized, 720 hour sunlight resistant, TW insulation compound also recommended for 75C Class 43 applications or outdoor jacket applications.Information provided by Georgia GulfGeorgia Gul.. |
|||
Volume Resistivity | 6.00e+14 ohm-cm | 6.00e+14 ohm-cm | ASTM D257 |
Fainplast Compounds Hax™ HF 213 Flame Retardant Polyolefin Cable Compound Thermoplastic halogen free flame retardant compound based on polyolefins and mineral fillersGrade description:General purpose, improved processabilityInformation provided by Fainplast Compounds |
|||
Volume Resistivity | 6.00e+14 ohm-cm | 6.00e+14 ohm-cm | Conditioned; ASTM D257 |
Solvay Specialty Polymers Amodel® AS-4145 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AS-4145 HS polyphthalamide (PPA) is a 45% glass reinforced resin that is hot-water moldable. Key properties include high heat resistance, high strength and stiffness over a broad temperature.. |