Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 4.00e+9 ohm-cm | 4.00e+9 ohm-cm | DIN 53482 |
DSM Fibre Intermediates Nyrim® 3000 (Conditioned) Conditioned at 23°C and 50% Relative Humidity.Nyrim is a Block Copolymer of Nylon 6 and an elastomer with exceptional properties in impact resistance, fatigue and abrasion resistance. Nyrim is proc.. |