Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 4.00e+15 ohm-cm | 4.00e+15 ohm-cm | ASTM D257 |
ExxonMobil Santoprene® 111-64 Thermoplastic Elastomer
(discontinued **) A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range .. |
|||
Volume Resistivity | 4.00e+15 ohm-cm | 4.00e+15 ohm-cm | |
Momentive Performance Materials N-Sil® RTV122 Silicone Modified Alkoxy Adhesive Sealants, White N-Sil® adhesive sealants are one-component, ready-to-use, and cure to a tough, resilient silicone rubber on exposure to atmospheric moisture at room temperature.Key Performance Properties: Primer.. |
|||
Volume Resistivity | 4.00e+15 ohm-cm | 4.00e+15 ohm-cm | |
Momentive Performance Materials N-Sil® RTV123 Silicone Modified Alkoxy Adhesive Sealants, Black N-Sil® adhesive sealants are one-component, ready-to-use, and cure to a tough, resilient silicone rubber on exposure to atmospheric moisture at room temperature.Key Performance Properties: Primer.. |
|||
Volume Resistivity | 4.00e+15 ohm-cm | 4.00e+15 ohm-cm | |
Momentive Performance Materials N-Sil® RTV128 Silicone Modified Alkoxy Adhesive Sealants, Translucent N-Sil® adhesive sealants are one-component, ready-to-use, and cure to a tough, resilient silicone rubber on exposure to atmospheric moisture at room temperature.Key Performance Properties: Primer.. |
|||
Volume Resistivity | 4.00e+15 ohm-cm | 4.00e+15 ohm-cm | Conditioned; IEC 60093 |
Lanxess Durethan® BKV 30 HTS 901510 Nylon 6, 30% Glass Fiber PA 6, injection molding grade, 30% glass fibers, very good heat-ageing resistance |
|||
Volume Resistivity | 4.00e+15 ohm-cm | 4.00e+15 ohm-cm | ASTM D257 |
SABIC Innovative Plastics NORYL WCP921A PPE-TPE Flexible Noryl* injection molding grade. Low specific gravity with good non-halogenated flame retardant performance. Developed for overmolding applications such as plugs, strain reliefs, and connect.. |
|||
Volume Resistivity | 4.00e+15 ohm-cm | 4.00e+15 ohm-cm | ASTM D257 |
SABIC Innovative Plastics NORYL WCP921A PPE-TPE (Asia Pacific) Flexible Noryl* injection molding grade. Low specific gravity with good non-halogenated flame retardant performance. Developed for overmolding applications such as plugs, strain reliefs, and connect.. |
|||
Volume Resistivity | 4.00e+15 ohm-cm | 4.00e+15 ohm-cm | ASTM D257 |
SABIC Innovative Plastics NORYL WCP921A PPE-TPE (Europe-Africa-Middle East) Flexible Noryl* injection molding grade. Low specific gravity with good non-halogenated flame retardant performance. Developed for overmolding applications such as plugs, strain reliefs, and connect.. |
|||
Volume Resistivity | 4.00e+15 ohm-cm | 4.00e+15 ohm-cm | IEC 93 |
Wolf Kunststoff ZEDEX® ZX-324V11T A3L PEEK Polymer, Reinforced Main Charactistics: Stress resistant; High impact strength at 196 ° C Applications: Shipbuilding; Chemical Engineering; Automitve Technology; Machine ToolsInformation provided by Zedex |
|||
Volume Resistivity | 4.00e+15 ohm-cm | 4.00e+15 ohm-cm | |
Tra-Con Tra-Cast 3012 Clear Epoxy Casting Compound TRA-CAST 3012 is a clear, low viscosity epoxy casting compound recommended for industrial embedding and casting applications where its combination of superior properties good clarity, long pot life,.. |
|||
Volume Resistivity | >= 4.00e+15 ohm-cm | >= 4.00e+15 ohm-cm | ASTM D257 |
Fainplast Compounds Hax™ HFX 509 Crosslinkable HFFR Cable Compound Polyolefin based HFFR silane grafted compound; cross-linkable by heat and moisture and by addition of suitable catalystGrade description:• Insulation for solar cablesInformation provided by Fainpla.. |
|||
Volume Resistivity | 4.00e+15 ohm-cm | 4.00e+15 ohm-cm | |
3M 941 Adhesive Transfer Tapes with Adhesive 100 These 3M™ Adhesive Transfer Tapes with 3M™ Adhesive 100 are designed for temperature exposure to 450°F (232°C) for short periods of time and/or solvent resistance. They have exceptional shear va.. |
|||
Volume Resistivity | 4.00e+15 ohm-cm | 4.00e+15 ohm-cm | |
3M 9461P Adhesive Transfer Tapes with Adhesive 100 These 3M™ Adhesive Transfer Tapes with 3M™ Adhesive 100 are designed for temperature exposure to 450°F (232°C) for short periods of time and/or solvent resistance. They have exceptional shear va.. |
|||
Volume Resistivity | 4.00e+15 ohm-cm | 4.00e+15 ohm-cm | |
3M 9461PC Adhesive Transfer Tapes with Adhesive 100 These 3M™ Adhesive Transfer Tapes with 3M™ Adhesive 100 are designed for temperature exposure to 450°F (232°C) for short periods of time and/or solvent resistance. They have exceptional shear va.. |
|||
Volume Resistivity | 4.00e+15 ohm-cm | 4.00e+15 ohm-cm | |
3M 965 Adhesive Transfer Tapes with Adhesive 100 These 3M™ Adhesive Transfer Tapes with 3M™ Adhesive 100 are designed for temperature exposure to 450°F (232°C) for short periods of time and/or solvent resistance. They have exceptional shear va.. |
|||
Volume Resistivity | 4.00e+15 ohm-cm | 4.00e+15 ohm-cm | |
3M 966 Adhesive Transfer Tapes with Adhesive 100 These 3M™ Adhesive Transfer Tapes with 3M™ Adhesive 100 are designed for temperature exposure to 450°F (232°C) for short periods of time and/or solvent resistance. They have exceptional shear va.. |
|||
Volume Resistivity | 4.00e+15 ohm-cm | 4.00e+15 ohm-cm | |
3M 9462P Adhesive Transfer Tapes with Adhesive 100 These 3M™ Adhesive Transfer Tapes with 3M™ Adhesive 100 are designed for temperature exposure to 450°F (232°C) for short periods of time and/or solvent resistance. They have exceptional shear va.. |
|||
Volume Resistivity | 4.00e+15 ohm-cm | 4.00e+15 ohm-cm | ASTM D257 |
Owens Corning Glass Fiber Reinforced Polyphenylene Sulfide, 40 wt.% glass Polyphenylene Sulfide provides excellent resistance to organic solvents (below 375°F). It is unaffected by strong alkalis or aqueous organic salt solutions. Data provided by the manufacturer, Owen.. |