Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 3.00e+16 ohm-cm | 3.00e+16 ohm-cm | ASTM D257 |
Samyang Triloy® 410 PC/PET alloy
(discontinued **) Characteristics:Impact resistantHeat resistantDimensional stabilityProcessabilityGood flowApplications:O/A partRear view mirror housingRice cooker baseAll information provided by Samyang |
|||
Volume Resistivity | 3.00e+16 ohm-cm | 3.00e+16 ohm-cm | ASTM D257 |
Samyang Triloy® 410N PC/PET alloy, Flame Retardant
(discontinued **) Characteristics:Impact resistantHeat resistantDimensional stabilityProcessabilityFlame retardantApplications:O/A partRear view mirror housingRice cooker baseAll information provided by Samyang |
|||
Volume Resistivity | 3.00e+16 ohm-cm | 3.00e+16 ohm-cm | ASTM D257 |
Solvay Specialty Polymers Udel® GF-110 Polysulfone (PSU)
(Unverified Data**) Udel GF-110, resin is a 10% glass fiber reinforced polysulfone (PSU). Glass fiber substantially increases the rigidity, tensile strength, creep resistance, dimensional stability and chemical resista.. |
|||
Volume Resistivity | 3.00e+16 ohm-cm | 3.00e+16 ohm-cm | measured 1 min. after applying DC 500 V; JIS K-6911 |
Kuraray SEPTON® S2063 Thermoplastic Rubber SEPTON® is a series of high performance thermoplastic rubbers developed by Kuraray Co. Ltd. using its isoprene technology. SEPTON® resins are hydrogenated styrenic block copolymers, which exhi.. |
|||
Volume Resistivity | 3.00e+16 ohm-cm | 3.00e+16 ohm-cm | ASTM D257 |
SABIC Innovative Plastics ULTEM 2300 PEI 30% Glass fiber filled, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. NSF 51 listing, WRAS certification, KTW certification in recognized colors. |
|||
Volume Resistivity | 3.00e+16 ohm-cm | 3.00e+16 ohm-cm | ASTM D257 |
SABIC Innovative Plastics ULTEM 2300 PEI (Asia Pacific) 30% Glass fiber filled, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. NSF 51 listing, WRAS certification, KTW certification in recognized colors. |
|||
Volume Resistivity | 3.00e+16 ohm-cm | 3.00e+16 ohm-cm | ASTM D257 |
SABIC Innovative Plastics ULTEM 2300F PEI 30% Glass fiber filled, standard flow Polyetherimide (Tg 217C). ECO Conforming. US FDA Food Contact compliant in recognized colors. |
|||
Volume Resistivity | 3.00e+16 ohm-cm | 3.00e+16 ohm-cm | ASTM D257 |
SABIC Innovative Plastics ULTEM 2300R PEI (Asia Pacific) 30% Glass fiber filled, standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing. |
|||
Volume Resistivity | 3.00e+16 ohm-cm | 3.00e+16 ohm-cm | ASTM D257 |
Solvay Specialty Polymers Udel® P-3500 LCD Polysulfone (PSU) Udel® P-3500 LCD is a very high molecular weight grade of polysulfone, and therefore offers the greatest toughness and chemical resistance of the available grades. It is well-suited for extrusion.. |
|||
Volume Resistivity | 3.00e+16 ohm-cm | 3.00e+16 ohm-cm | ASTM D257 |
Techmer ES HiFill® PBT GF20 BK007 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightAppearance: BlackTPCI# 6225111Information provided by TP Composites, Inc. |
|||
Volume Resistivity | 3.00e+16 ohm-cm | 3.00e+16 ohm-cm | ASTM D257 |
Techmer ES HiFill® PBT GF40 40% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Volume Resistivity | 3.00e+16 ohm-cm | 3.00e+16 ohm-cm | ASTM D257 |
Techmer ES HiFill® PP E GF40 CC 40% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightAdditive: Heat StabilizerFeatures: Chemically Coupled, Heat Stabilized and High Viscosit.. |
|||
Volume Resistivity | 3.00e+16 ohm-cm | 3.00e+16 ohm-cm | ASTM D257 |
Techmer ES HiFill® PP GF30 TL15 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: PTFE Lubricant (15%)Features: LubricatedInformation provided by TP Composites.. |
|||
Volume Resistivity | 3.00e+16 ohm-cm | 3.00e+16 ohm-cm | ASTM D257 |
Techmer ES HiFill® PP GF40 CC 40% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightFeatures: Chemically CoupledInformation provided by TP Composites, Inc. |
|||
Volume Resistivity | 3.00e+16 ohm-cm | 3.00e+16 ohm-cm | ASTM D257 |
Techmer ES Luriblend® PBT GB30 TL15 30% Glass Bead Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Bead, 30% Filler by WeightAdditive: PTFE LubricantFeatures: LubricatedInformation provided by TP Composites, Inc. |
|||
Volume Resistivity | 3.00e+16 ohm-cm | 3.00e+16 ohm-cm | ASTM D257 |
Solvay Specialty Polymers Udel® P-1700 Polysulfone (PSU) Udel® P-1700 polysulfone (PSU) is a tough, rigid, high-strength thermoplastics suitable for continuous use up to 300°F (149°C). It is resistant to oxidation and hydrolysis and withstand pro.. |
|||
Volume Resistivity | 3.00e+16 ohm-cm | 3.00e+16 ohm-cm | ASTM D257 |
Techmer ES HiFill® PBT GF10 CBA 10% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 10% Filler by WeightFeatures: FoamableAppearance: Natural ColorInformation provided by TP Composites, Inc. |
|||
Volume Resistivity | 3.00e+16 ohm-cm | 3.00e+16 ohm-cm | ASTM D257 |
Techmer ES HiFill® PBT GF15 15% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 15% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Volume Resistivity | 3.00e+16 ohm-cm | 3.00e+16 ohm-cm | ASTM D257 |
Techmer ES HiFill® PBT GF15 BK001 15% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 15% Filler by WeightUL File Number: E157318Appearance: BlackTPCI# 6100111Information provided by TP Composit.. |
|||
Volume Resistivity | 3.00e+16 ohm-cm | 3.00e+16 ohm-cm | ASTM D257 |
Techmer ES HiFill® PBT GF15 WT 096 LE 15% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 15% Filler by WeightUL File Number: E157318Appearance: WhiteTPCI# 6862111Information provided by TP Composit.. |
|||
Volume Resistivity | 3.00e+16 ohm-cm | 3.00e+16 ohm-cm | ASTM D257 |
Techmer ES HiFill® PBT GF20 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Volume Resistivity | 3.00e+16 ohm-cm | 3.00e+16 ohm-cm | ASTM D257 |
Westlake Plastics Tempalux® 30% GF Polyetherimide An amorphous thermoplastic polyetherimide, stock shapes from ULTEM® resin possess a combination of useful characteristics, including high strength at elevated temperatures, high modulus, and broad .. |
|||
Volume Resistivity | 3.00e+16 ohm-cm | 3.00e+16 ohm-cm | IEC 60093 |
Polyplastics Duranex® 3116 Polybutylene Terephthalate (PBT), Standard, FR, UL approved regrind 50%, 7.5% GF filled DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Volume Resistivity | 3.00e+16 ohm-cm | 3.00e+16 ohm-cm | IEC 60093 |
Polyplastics Duranex® 3405 Polybutylene Terephthalate (PBT), Standard, 45% GF filled DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Volume Resistivity | >= 3.00e+16 ohm-cm | >= 3.00e+16 ohm-cm | ASTM D257 |
Fainplast Compounds Ethylplus 615 MD Polyethylene Cable Compound Polyethelene, halogen-free cable compound with superior thermo-mechanical properties, outstanding heat resistance, and high electrical propertiesSolid MDPEInformation provided by Fainplast Compounds.. |
|||
Volume Resistivity | 3.00e+16 ohm-cm | 3.00e+16 ohm-cm | |
Asahi Glass AFLAS® 100H TFE/P Fluoroelastomer AFLAS® 100/150 fluoroelastomers are alternating copolymers of tetrafluoroethylene and propylene. They offer 1) excellent heat resistance, 2) exceptional chemical resistance especially to bases and .. |
|||
Volume Resistivity | 3.00e+16 ohm-cm | 3.00e+16 ohm-cm | |
Asahi Glass AFLAS® 150P TFE/P Fluoroelastomer AFLAS® 100/150 fluoroelastomers are alternating copolymers of tetrafluoroethylene and propylene. They offer 1) excellent heat resistance, 2) exceptional chemical resistance especially to bases and .. |
|||
Volume Resistivity | 3.00e+16 ohm-cm | 3.00e+16 ohm-cm | ASTM D257 |
Samyang Triloy® S460G15 Polymer Alloy, Reinforced Excellent impact, formability and weather resistance.220 is a reinforced grade.Applications: LCD Panel Frame - for dimensional stabilityInformation provided by Samyang. |
|||
Volume Resistivity | 3.00e+16 ohm-cm @Temperature 23.0 °C |
3.00e+16 ohm-cm @Temperature 73.4 °F |
IEC 60093 |
DuPont Performance Polymers Sorona® 3015G BK001 Polytrimethylene Terephthalate (PTT)
(Unverified Data**)& Sorona® 3015G BK001 is a 15% glass reinforced black PTT resin containing 31% renewably sourced ingredients by weight (37% polymer basis) with good strength, stiffness and low warpage and superior s.. |
|||
Volume Resistivity | 3.00e+16 ohm-cm | 3.00e+16 ohm-cm | ASTM D257 |
Quantum PEI - Ultem® 30% Glass Fiber Filled Information provided by Quantum Advanced Engineering Plastics |