Polymer Property : Volume Resistivity = 2.90e+15 ohm-cm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Volume Resistivity 2.90e+15 ohm-cm

@Temperature 23.0 °C
2.90e+15 ohm-cm

@Temperature 73.4 °F
50% RH, ASTM D257-07; ASTM D257
PolyOne OnFlex™ HFFR 310-01 Thermoplastic Elastomer (TPE)
OnFlex™ HFFR 310-01 is a non-halogen flame retardant material designed for cable jackets. New Product. Commercial specifications have not been established. - Non-halogen flame retardant - UL62 comp..
Volume Resistivity 2.90e+15 ohm-cm

@Temperature 23.0 °C
2.90e+15 ohm-cm

@Temperature 73.4 °F
50%RH, ASTM D257-07; ASTM D257
PolyOne OnFlex™ HFFR 315-01 Thermoplastic Elastomer (TPE)
OnFlex™ HFFR 315-01 a is non-halogen flame retardant material designed for flexible power cord insulation, cable jackets, and ribbon cables. New Product. Commercial specifications have not been est..
Volume Resistivity 2.90e+15 ohm-cm

@Temperature 23.0 °C
2.90e+15 ohm-cm

@Temperature 73.4 °F
50% RH, ASTM D257-07; ASTM D257
PolyOne OnFlex™ HFFR 320-01 Thermoplastic Elastomer (TPE)
OnFlex™ HFFR 320-01 is a non-halogen flame retardant material designed for flexible power cord insulation and cable jackets. New Product. Commercial specifications have not been established. - Non-..
Volume Resistivity 2.90e+15 ohm-cm
2.90e+15 ohm-cm
ASTM D257
PolyOne Geon™ Vinyl Flexible R3792E Polyvinyl Chloride, Flexible (PVC, Flexible)
Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne
Volume Resistivity 2.90e+15 ohm-cm
2.90e+15 ohm-cm
ASTM D257
Ensinger Tecatron® XP-64 Compression Molded PPS Compound, 40% Fiberglass
Ensinger Special Polymers has over twenty different grades of TECATRON PPS available. Custom formulations can be blended to suit specific applications. Compression molding is amenable to short run p..