Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 2.30e+16 ohm-cm | 2.30e+16 ohm-cm | ASTM D257 |
SABIC Innovative Plastics NORYL SE1X PPE+PS PPE+PS blend. Unfilled. Non-brominated, non-chlorinated FR system. UL94 V1, UL746C F1. Dielectric strength. Suitable for E/E market indoor/outdoor applications. |
|||
Volume Resistivity | 2.30e+16 ohm-cm | 2.30e+16 ohm-cm | ASTM D257 |
SABIC Innovative Plastics NORYL SE1X PPE+PS (Asia Pacific) PPO+PS. Improved productivity and reliability. Nonchlorinated, nonbrominated flame retardant. 244F HDT. |
|||
Volume Resistivity | 2.30e+16 ohm-cm | 2.30e+16 ohm-cm | GB/T1410-2006 |
Sichuan Deyang Haton® hGR31M1 Polyphenylene Sulfide Injection moldingInformation provided by Sichuan Deyang Chemical Co., LTD |
|||
Volume Resistivity | 2.30e+16 ohm-cm | 2.30e+16 ohm-cm | IEC 60093 |
Lanxess Pocan® BFN 4231 000000 PBT, 25% Glass Fiber PBT, 25% glass fibers, injection molding, halogen free flame retardantInformation provided by LANXESS. |