Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 2.00e+14 ohm-cm | 2.00e+14 ohm-cm | ASTM D257 |
Rogers Corporation TMM® TMM10 Ceramic Thermoset Polymer Composite TMM® Thermoset microwave materials are ceramic thermoset polymer composites designed for high plate-thru-hole reliability stripline and microstrip applications. The electrical and mechanical prope.. |
|||
Volume Resistivity | 2.00e+14 ohm-cm | 2.00e+14 ohm-cm | ASTM D257 |
Rogers Corporation TMM® TMM101 Ceramic Thermoset Polymer Composite TMM® Thermoset microwave materials are ceramic thermoset polymer composites designed for high plate-thru-hole reliability stripline and microstrip applications. The electrical and mechanical prope.. |
|||
Volume Resistivity | 2.00e+14 ohm-cm | 2.00e+14 ohm-cm | wet; ASTM D257 |
S&E Specialty Polymers GA-1050-OR3-LF PVC Application: Lead free, 105° C PVC insulating compound designed for SJEOO applications. Complies with RoHS requirements.Information provided by S&E Specialty Polymers |
|||
Volume Resistivity | 2.00e+14 ohm-cm | 2.00e+14 ohm-cm | |
ACC QSil 30 QSI Quantum Silicones 50 Durometer Condensation Cure for Potting
(discontinued **) Part of the Amber Chemical Group. Data provided by manufacturer.Characteristics: self-leveling, variable cure speeds, excellent thermal properties, 100% solid. |
|||
Volume Resistivity | 2.00e+14 ohm-cm | 2.00e+14 ohm-cm | |
Momentive Performance Materials RTV511 Silicone Rubber Compound for Low Temperature Potting, Encapsulating and Sealing, White RTV511, RTV560 and RTV577 silicone rubber compounds are low temperature two-part silicone elastomers. They are supplied ready to use with a base compound and DEBT (deputy tin deflagrate) as the stan.. |
|||
Volume Resistivity | 2.00e+14 ohm-cm | 2.00e+14 ohm-cm | |
Momentive Performance Materials RTV560 Silicone Rubber Compound for Low Temperature Potting, Encapsulating and Sealing, Red RTV511, RTV560 and RTV577 silicone rubber compounds are low temperature two-part silicone elastomers. They are supplied ready to use with a base compound and DBT (dibutyl tin dilaurate) as the stand.. |
|||
Volume Resistivity | 2.00e+14 ohm-cm | 2.00e+14 ohm-cm | ASTM D257 |
Techmer ES Elastoblend® PA6/6 IM L W Nylon 66 Availability: North AmericaForms: PelletsAdditive: Lubricant and Impact ModifierFeatures: Lubricant and Impact ModifiedProcessing Method: Injection MoldingInformation provided by TP Composites, Inc... |
|||
Volume Resistivity | 2.00e+14 ohm-cm | 2.00e+14 ohm-cm | ASTM D257 |
Unitika P-5001 Engineering Plastic P series resins are resins succeeding the characteristics of the neat polymer, U100, and improved in flowability and optical properties. Among many super engineering plastics, the resins are few tra.. |
|||
Volume Resistivity | 2.00e+14 ohm-cm | 2.00e+14 ohm-cm | ASTM D257 |
Westlake Plastics Ardel® Polyarylate Stock shapes extruded from Ardel resin are specifically formulated to endure the damaging effects of UV light. When exposed to UV light, this unique material undergoes a molecular rearrangement res.. |
|||
Volume Resistivity | 2.00e+14 ohm-cm | 2.00e+14 ohm-cm | IEC 93 |
Wolf Kunststoff ZEDEX® ZX-100K A1K Polymer Alloy Main Characteristics: Hard; Stiff; Tough; High fatigue strength; Good weather resistance; Good machinability; FDA compliant LABS; PTFE and silicone-free; KTW approved; Stress resistantApplications: .. |
|||
Volume Resistivity | 2.00e+14 ohm-cm | 2.00e+14 ohm-cm | IEC 93 |
Wolf Kunststoff ZEDEX® ZX-100MT A1T Polymer Alloy, Mineral Reinforced Stiff; Hard; Very high strength; No fiber reinforcementApplications: Handling, Vessel and Pump, Steel and Water, Chemical Engineering, Automotive Technology, Machine ToolsInformation provided by Zed.. |
|||
Volume Resistivity | 2.00e+14 ohm-cm | 2.00e+14 ohm-cm | |
Tra-Con Tra-Bond 789-3 Moisture Resistant Adhesive TRA-BOND 789-3 one component, high strength toughened adhesive is designed for microelectronic applications, including substrate attach and package sealing, which require good moisture resistance. I.. |
|||
Volume Resistivity | 2.00e+14 ohm-cm | 2.00e+14 ohm-cm | ASTM D257 |
Unitika P-1001A Engineering Plastic P series resins are resins succeeding the characteristics of the neat polymer, U100, and improved in flowability and optical properties. Among many super engineering plastics, the resins are few tra.. |
|||
Volume Resistivity | 2.00e+14 ohm-cm | 2.00e+14 ohm-cm | IEC 60093 |
Polyplastics Duracon® TD-15 Acetal Co-polymer (POM), High impact, Flexible DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |
|||
Volume Resistivity | 2.00e+14 ohm-cm | 2.00e+14 ohm-cm | |
Tra-Con Tra-Bond 2105 Clear Rigid, Medium Viscosity Epoxy Adhesive TRA-BOND 2105 is a clear, medium viscosity epoxy adhesive which contains no solvents or other additives which can be harmful to the environment or to its users. It has excellent adhesion to glass, c.. |
|||
Volume Resistivity | 2.00e+14 ohm-cm | 2.00e+14 ohm-cm | cond; IEC 60093 |
DSM EcoPaXX® Q-X07209 PA410-I-GF40 % Glass Reinforced, Impact Modified |
|||
Volume Resistivity | 2.00e+14 ohm-cm @Temperature 23.0 °C |
2.00e+14 ohm-cm @Temperature 73.4 °F |
ASTM D257 |
Fainplast Compounds FK 91 Flexible PVC, Insulation Lead Free Power cables |
|||
Volume Resistivity | 2.00e+14 ohm-cm @Temperature 23.0 °C |
2.00e+14 ohm-cm @Temperature 73.4 °F |
ASTM D257 |
Fainplast Compounds FR 95 Flexible PVC, Insulation Power cables |
|||
Volume Resistivity | 2.00e+14 ohm-cm @Temperature 23.0 °C |
2.00e+14 ohm-cm @Temperature 73.4 °F |
ASTM D257 |
Fainplast Compounds HLA 075 Flexible PVC, Insulation for High Temperatures Operating temperature 105°C |
|||
Volume Resistivity | 2.00e+14 ohm-cm | 2.00e+14 ohm-cm | IEC 60093 |
DSM Akulon® K224-HG4 Nylon 6-20% Glass Reinforced (European Grade) (Cond) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Volume Resistivity | 2.00e+14 ohm-cm @Temperature 23.0 °C |
2.00e+14 ohm-cm @Temperature 73.4 °F |
ASTM D257 |
Fainplast Compounds KL 84/1 Flexible PVC, Insulation for High Temperatures Lead Free General purposes flame retardant |
|||
Volume Resistivity | 2.00e+14 ohm-cm @Temperature 23.0 °C |
2.00e+14 ohm-cm @Temperature 73.4 °F |
ASTM D257 |
Fainplast Compounds KL 92/3 Flexible PVC, Insulation for High Temperatures Lead Free Operatine temperature 105°C |
|||
Volume Resistivity | 2.00e+14 ohm-cm | 2.00e+14 ohm-cm | 50% RH, 500V; ASTM D257 |
ALM PA-616-GS Filled Nylon 12 Prototyping Polymer 50% glass sphere filled material for improved dimensional stability, increased stiffness, and higher temperature applications when compared to unfilled PA.The PA 616-GS can be processed on any laser.. |
|||
Volume Resistivity | 2.00e+14 ohm-cm | 2.00e+14 ohm-cm | |
Atom Adhesives AA-BOND FDA15 Epoxy Adhesive AA-BOND FDA15 is a low viscosity epoxy resin system specifically developed for bonding and coating applications in accordance with Title 21, U.S. Code of Federal Regulations, Food and Drug Administr.. |
|||
Volume Resistivity | 2.00e+14 ohm-cm @Temperature 20.0 °C |
2.00e+14 ohm-cm @Temperature 68.0 °F |
65% RH; ASTM D257 |
Arkema Group KYNAR® 740 Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeabili.. |
|||
Volume Resistivity | 2.00e+14 ohm-cm @Temperature 20.0 °C |
2.00e+14 ohm-cm @Temperature 68.0 °F |
65% RH; ASTM D257 |
Arkema Group KYNAR® 760 Polyvinylidene Fluoride Homopolymer - Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeabili.. |
|||
Volume Resistivity | 2.00e+14 ohm-cm | 2.00e+14 ohm-cm | DC, 65% RH; ASTM D257 |
Arkema Group Kynar Super Flex® 2500 PVDF Copolymer
(discontinued **) Copolymer Series, Kynar® components are used extensively in the high purity semiconductor market, the pulp and paper industry, nuclear waste processing, and the general chemical processing industry.. |