Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | >= 1.0e+14 ohm-cm | >= 1.0e+14 ohm-cm | IEC 60093 |
Quadrant EPP Borotron® UH PE-UHMW + boron based additive (ISO Data) Borotron UH and Borotron HM are boron loaded PE-(U)HMW grades, specifically developed for neutron shielding purposes in nuclear installations. The high hydrogen content of PE-(U)HMW makes it very su.. |
|||
Volume Resistivity | >= 1.0e+14 ohm-cm | >= 1.0e+14 ohm-cm | IEC 60093 |
Quadrant EPP Ertacetal® H POM-H, extruded (ISO Data) Ertacetal H is Quadrant’s homopolymer acetal grade. It offers a higher mechanical strength, stiffness, hardness and creep resistance as well as a lower thermal expansion rate and often also a bette.. |
|||
Volume Resistivity | >= 1.0e+14 ohm-cm | >= 1.0e+14 ohm-cm | IEC 60093 |
Quadrant EPP Ertalon® 4.6 PA 4.6, extruded (ISO Data) Compared with conventional nylons, Ertalon 4.6 features a better retention of stiffness and creep resistance over a wide range of temperatures as well as superior heat ageing resistance. Therefore, .. |
|||
Volume Resistivity | >= 1.0e+14 ohm-cm | >= 1.0e+14 ohm-cm | IEC 60093 |
Quadrant EPP Ertalon® 6 PLA PA 6, cast (ISO Data) Unmodified cast nylon 6 grade exhibiting characteristics which come very close to those of Ertalon 66 SA. It combines high strength, stiffness and hardness with good creep and wear resistance, heat .. |
|||
Volume Resistivity | >= 1.0e+14 ohm-cm | >= 1.0e+14 ohm-cm | IEC 60093 |
Quadrant EPP Ertalon® 66 GF30 PA 66, 30% glass filled, extruded (ISO Data) Compared with virgin PA 66, this 30 % glass fibre reinforced and heat stabilised nylon grade offers increased strength, stiffness, creep resistance and dimensional stability whilst retaining an exce.. |
|||
Volume Resistivity | >= 1.0e+14 ohm-cm | >= 1.0e+14 ohm-cm | IEC 60093 |
Quadrant EPP Ertalon® 66 SA PA 66, extruded (ISO Data) Material with a higher mechanical strength, stiffness, heat and wear resistance than Ertalon 6 SA. It also has a better creep resistance but its impact strength and mechanical damping ability is red.. |
|||
Volume Resistivity | >= 1.0e+14 ohm-cm | >= 1.0e+14 ohm-cm | IEC 60093 |
Quadrant EPP Ertalon® 6XAU+ PA 6, heat stabilized, cast (ISO Data) Ertalon 6 XAU+ is a heat stabilized cast nylon grade with a very dense and highly crystalline structure. Compared with conventional extruded or cast nylons, Ertalon 6 XAU+ offers superior heat agein.. |
|||
Volume Resistivity | >= 1.0e+14 ohm-cm | >= 1.0e+14 ohm-cm | IEC 60093 |
Quadrant EPP Ertalyte® PET, cast (ISO Data) The specific properties of this virgin crystalline PET make it especially suitable for the manufacture of mechanical precision parts which have to sustain high loads and/or are subject to wear. |
|||
Volume Resistivity | >= 1.0e+14 ohm-cm | >= 1.0e+14 ohm-cm | IEC 60093 |
Quadrant EPP Ertalyte® TX PET + solid lubricant, extruded (ISO Data) Ertalyte TX is a polyethylene terephthalate compound incorporating a uniformly dispersed solid lubricant. Its specific formulation makes it a premium internally lubricated bearing-grade. Ertalyte TX.. |
|||
Volume Resistivity | >= 1.0e+14 ohm-cm | >= 1.0e+14 ohm-cm | IEC 60093 |
Quadrant EPP Ketron® 1000 PEEK unfilled, extruded (ISO Data) Ketron PEEK-1000 stock shapes are produced from virgin polyetheretherketone resin and offer the highest toughness and impact strength of all Ketron PEEK grades. Both Ketron PEEK-1000 natural & black.. |
|||
Volume Resistivity | >= 1.0e+14 ohm-cm | >= 1.0e+14 ohm-cm | IEC 60093 |
Quadrant EPP Nylatron® GS PA 6 + MoS2, extruded (ISO Data) The addition of MoS2 renders this material somewhat stiffer, harder and dimensionally more stable than Ertalon 66 SA, but results in some loss of impact strength. The nucleating effect of the molybd.. |
|||
Volume Resistivity | >= 1.0e+14 ohm-cm | >= 1.0e+14 ohm-cm | IEC 60093 |
Quadrant EPP Nylatron® GSM PA 6 + MoS2, cast (ISO Data) Nylatron GSM contains finely divided particles of molybdenum disulphide to enhance its bearing and wear behaviour without impairing the impact and fatigue resistance inherent to unmodified cast nylo.. |
|||
Volume Resistivity | >= 1.0e+14 ohm-cm | >= 1.0e+14 ohm-cm | IEC 60093 |
Quadrant EPP Nylatron® MC901 PA 6, blue, cast (ISO Data) This modified cast nylon 6 grade with its distinctive blue colour exhibits higher toughness, flexibility and fatigue resistance than Ertalon 6 PLA. It has proved to be an excellent material for gear.. |
|||
Volume Resistivity | >= 1.0e+14 ohm-cm | >= 1.0e+14 ohm-cm | IEC 60093 |
Quadrant EPP Nylatron® NSM PA 6 + internal lubricant, cast (ISO Data) Nylatron NSM is a proprietary cast nylon 6 formulation containing solid lubricant additives which grant this materials self-lubricity, excellent frictional behaviour, superior wear resistance and ou.. |
|||
Volume Resistivity | >= 1.0e+14 ohm-cm | >= 1.0e+14 ohm-cm | IEC 60093 |
Quadrant EPP PE 500 PE-HMW, virgin (ISO Data) This grade exhibits a good combination of stiffness, toughness, mechanical damping ability with wear- and abrasion resistance and can easily be welded. In less demanding applications with respect to.. |
|||
Volume Resistivity | >= 1.0e+14 ohm-cm | >= 1.0e+14 ohm-cm | IEC 60093 |
Quadrant EPP Quadrant PPSU unfilled, extruded (ISO Data) Quadrant PPSU is a black, amorphous high performance thermoplastic, offering better impact strength and chemical resistance than polysulfone and polyetherimide. Quadrant PPSU also has superior hydro.. |
|||
Volume Resistivity | >= 1.0e+14 ohm-cm | >= 1.0e+14 ohm-cm | IEC 60093 |
Quadrant EPP Symalit® 1000 ECTFE, unfilled, lining industries (ISO Data) Symalit 1000 ECTFE is made from a fluoropolymer resin that is a copolymer of ethylene and chlorotrifluoroethylene. It exhibits good mechanical properties combined with an excellent chemical resistan.. |
|||
Volume Resistivity | >= 1.0e+14 ohm-cm | >= 1.0e+14 ohm-cm | IEC 60093 |
Quadrant EPP Techtron® HPV PPS + solid lubricant, bearing grade, extruded (ISO Data) As a reinforced, internally lubricated PPS grade, Techtron HPV PPS demonstrates an excellent combination of properties including wear resistance, load-bearing capabilities and dimensional stability .. |
|||
Volume Resistivity | >= 1.0e+14 ohm-cm | >= 1.0e+14 ohm-cm | IEC 60093 |
Quadrant EPP Techtron® PPS unfilled, extruded (ISO Data) This unfilled polyphenylene sulfide based material is ideal for structural applications in corrosive environments or as a PEEK replacement at less demanding temperatures. Very good dimensional stabi.. |
|||
Volume Resistivity | >= 1.0e+14 ohm-cm | >= 1.0e+14 ohm-cm | IEC 60093 |
Quadrant EPP TIVAR® 1000 PE-UHMW, virgin (ISO Data) TIVAR 1000 exhibits a very well balanced property profile. It combines a very good wear and abrasion resistance with an outstanding impact strength, even at temperatures below -200°C. |
|||
Volume Resistivity | >= 1.0e+14 ohm-cm | >= 1.0e+14 ohm-cm | IEC 60093 |
Quadrant EPP TIVAR® Ceram P PE-UHMW + micro glass beads + other additives (ISO Data) TIVAR Ceram P is a wear improved PE-UHMW material with incorporated micro glass beads, specifically developed for use in the dewatering zone of paper machinery equipped with plastic wires and manufa.. |
|||
Volume Resistivity | >= 1.0e+14 ohm-cm | >= 1.0e+14 ohm-cm | IEC 60093 |
Quadrant EPP TIVAR® H.O.T. PE-UHMW + specific additives (ISO Data) TIVAR H.O.T. [Higher Operating Temperature] is formulated to maintain inherent PE-UHMW key properties over an extended service temperature range, in this way considerably increasing part life in low.. |
|||
Volume Resistivity | >= 1.0e+14 ohm-cm | >= 1.0e+14 ohm-cm | IEC 60093 |
Quadrant EPP TIVAR® MD PE-UHMW + metal detectable additive (ISO Data) This PE-UHMW grade with extremely high degree of polymerisation contains a metal detectable additive which does hardly affect the inherent PE-UHMW key properties. TIVAR MD presents excellent toughne.. |
|||
Volume Resistivity | >= 1.0e+14 ohm-cm | >= 1.0e+14 ohm-cm | IEC 60093 |
Quadrant EPP TIVAR® Oil Filled PE-UHMW + oil (ISO Data) TIVAR Oil Filled is a self-lubricating PE-UHMW material in the real meaning of the word. Next to an enhanced wear resistance, the incorporated and evenly dispersed oil renders this material a consid.. |
|||
Volume Resistivity | >= 1.0e+14 ohm-cm | >= 1.0e+14 ohm-cm | IEC 60093 |
Quadrant EPP Duratron® PBI CU60 compression moulded (ISO Data) Duratron CU60 PBI is very “clean” in terms of ionic impurity and does not outgas (except water). These characteristics make this material extremely attractive to high-tech industries such as semic.. |
|||
Volume Resistivity | 1.0e+14 - 1.0e+16 ohm-cm | 1.0e+14 - 1.0e+16 ohm-cm | IEC 60093 |
SABIC Innovative Plastics NORYL NH7111E PPE+HIPS Noryl* EXNL0280 is a glass fiber reinforced, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and low warpage, this resin also uses non-halogenated FR a.. |
|||
Volume Resistivity | 1.0e+14 - 1.0e+16 ohm-cm | 1.0e+14 - 1.0e+16 ohm-cm | IEC 60093 |
SABIC Innovative Plastics NORYL NH7111E PPE+HIPS (Asia Pacific) Noryl* EXNL0280 is a glass fiber reinforced, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and low warpage, this resin also uses non-halogenated FR a.. |
|||
Volume Resistivity | 1.0e+14 ohm-cm | 1.0e+14 ohm-cm | ASTM D257 |
Ensinger Tecaform™ FG Blue Food Grade Acetal (POM) Tecaform™ is resistant to hot water and typical cleaning chemicals. It possesses good bearing and wear properties. The blue color makes it more visible than standard grades. It is commonly used .. |
|||
Volume Resistivity | >= 1.0e+14 ohm-cm | >= 1.0e+14 ohm-cm | IEC 60093 |
Quadrant EPP Ketron® GF30 PEEK + glassfibres, extruded (ISO Data) This 30 % glass fibre reinforced grade offers a higher stiffness and creep resistance than Ketron PEEK-1000 and has a much better dimensional stability. This grade is very appropriate for structural.. |
|||
Volume Resistivity | >= 1.0e+14 ohm-cm | >= 1.0e+14 ohm-cm | IEC 60093 |
Quadrant EPP Quadrant PSU unfilled, extruded (ISO Data) Quadrant 1000 PSU is a slightly yellow, translucent (non-optical quality) amorphous thermoplastic material, offering a combination of excellent mechanical, thermal and electrical properties. It ofte.. |