Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 1.00e+8 ohm-cm | 1.00e+8 ohm-cm | ASTM D257 |
Gharda Chemicals G-PAEK™ 1200FCM Ultra High Performance PEK Polymer
(discontinued **) Milled carbon fiber reinforced in Poly Aryl Ether Ketone, semi-crystalline granules suitable for injection molding, easy flow, Black in colorApplication Areas: Suitable for high temperature applica.. |
|||
Volume Resistivity | 1.00e+8 ohm-cm | 1.00e+8 ohm-cm | ASTM D257 |
Kolon Kocetal® DP301 Modified Grade Acetal Copolymer
(discontinued **) Thermal properties: Kocetal has excellent heat stability; heat degradation is little under long term and high temperature application, compared to other POM. Maximum applicable temperature of produ.. |
|||
Volume Resistivity | 1.00e+8 ohm-cm | 1.00e+8 ohm-cm | ASTM D257 |
LG Chemical LUCON PN9009 PPS+MF Injection Molding Grade, PPS+MF, High Thermal Conductivity, Chemical Resistance, High Heat ResistanceApplication: Electrical or Electronic Parts (Heat sink, LED etc.) Motor HousingCAS No. 25212-74-2.. |
|||
Volume Resistivity | 1e+05 - 1.00e+8 ohm-cm | 1e+05 - 1.00e+8 ohm-cm | ASTM D257 |
Techmer ES Electrablend® PA6/6 C10 BK 10% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber Reinforcement, 10% Filler by WeightFeatures: ConductiveAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Volume Resistivity | 1e+05 - 1.00e+8 ohm-cm | 1e+05 - 1.00e+8 ohm-cm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-KON DX05301C PC (Asia Pacific) Low Ionic, Low Outgassing, Low LPC and ESD safe Polycarbonate compound suitable for Semiconductor and Hard Disk Drive (HDD) application.Added features of this material include: Clean Compounding Sys.. |
|||
Volume Resistivity | 1.00e+8 - 1.00e+10 ohm-cm | 1.00e+8 - 1.00e+10 ohm-cm | ASTM D257 |
SABIC Innovative Plastics LNP STAT-LOY KX09024 ACETAL COPOLYMER (Europe-Africa-Middle East) LNP* Statloy* KX09024 is a compound based on Polyacetal with reduced Resistivity. Added features include: Antistatic Properties |
|||
Volume Resistivity | 1.00e+8 - 1.00e+11 ohm-cm | 1.00e+8 - 1.00e+11 ohm-cm | ASTM D257 |
Techmer ES Statiblend® HIPS E Availability: North AmericaForms: PelletsAdditive: AntistaticFeatures: Antistatic and ConductiveAppearance: Natural ColorProcessing Method: ExtrusionInformation provided by TP Composites, Inc. |
|||
Volume Resistivity | 1.00e+8 - 1.00e+11 ohm-cm | 1.00e+8 - 1.00e+11 ohm-cm | ASTM D257 |
Techmer ES Statiblend® PA6/6 GF10 BK 10% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 10% Filler by WeightAdditive: LubricantFeatures: Conductive and LubricatedAppearance: BlackInformation provided by TP Comp.. |
|||
Volume Resistivity | 1.00e+8 - 1.00e+9 ohm-cm | 1.00e+8 - 1.00e+9 ohm-cm | Practical Use (Water Absorption 1.8%); ASTM-D257 |
Toyobo GLAMIDE® T-422VOR Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Volume Resistivity | 1.00e+8 - 1.00e+9 ohm-cm | 1.00e+8 - 1.00e+9 ohm-cm | Practical Use (Water Absorption 3.5%); ASTM-D257 |
Toyobo GLAMIDE® T-802 Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Volume Resistivity | 1.00e+8 ohm-cm | 1.00e+8 ohm-cm | |
Cotronics Duralco™ 4540 Machinable Epoxy Patches, fills, seals, and repairs with outstanding adhesion, ductility, thermal conductivity and shock resistance.Corrosion Resistance: excellent resistance to chemicals and solventsApplications: .. |
|||
Volume Resistivity | 1.00e+8 ohm-cm | 1.00e+8 ohm-cm | |
Cotronics Resbond™ 904 Ultra Temp Zirconia Adhesive and Coating Ultra Temp 904 is a smooth creamy paste that is easily brushed on ceramics, graphite, metals, etc. to form adhesive bonds and coatings that will withstand 4000°F (2200°C) continuous heat. It has .. |
|||
Volume Resistivity | 1.00e+8 ohm-cm | 1.00e+8 ohm-cm | IEC 60093 |
DSM Stanyl® 46HF5040 (COND) Nylon 46 40% Glass Reinforced, Heat Stabilized, Flame Retardant, High Flow (North America) Information provided by DSM Engineering Plastics. |
|||
Volume Resistivity | 1.00e+8 ohm-cm | 1.00e+8 ohm-cm | IEC 60093 |
DSM Stanyl® TE250F6 (COND) Nylon 46 30% Glass Reinforced, Heat Stabilized, Flame Retardant (North America) Information provided by DSM Engineering Plastics. |
|||
Volume Resistivity | 1.00e+8 ohm-cm | 1.00e+8 ohm-cm | IEC 60093 |
DSM Stanyl® TE250F9 (COND) Nylon 46 45% Glass Reinforced, Heat Stabilized, Flame Retardant (North America) Information provided by DSM Engineering Plastics. |
|||
Volume Resistivity | 1.00e+8 ohm-cm | 1.00e+8 ohm-cm | dry; IEC 60093 |
EMS-Grivory Grivory® BS EC PA6 Product description: Grilon BS 23 is an unreinforced, low viscosity and fine crystalline PA 6 injection molding grade. Grilon BS 23 has the following important properties: Good flow behaviorEasy pro.. |
|||
Volume Resistivity | 1.00e+8 ohm-cm | 1.00e+8 ohm-cm | IEC 60093 |
DSM Stanyl® TW200F8 (COND) Nylon 46 40% Glass Reinforced, Heat Stabilized (North America) Information provided by DSM Engineering Plastics. |
|||
Volume Resistivity | 1.00e+8 ohm-cm | 1.00e+8 ohm-cm | IEC 60093 |
DSM Stanyl® TW241F10 (COND) Nylon 46 50% Glass Reinforced, Heat Stabilized (North America) Information provided by DSM Engineering Plastics. |
|||
Volume Resistivity | 1.00e+8 ohm-cm | 1.00e+8 ohm-cm | IEC 60093 |
DSM Stanyl® TW250F6 Nylon 46-30% Glass Reinforced (European Grade) (Cond) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Volume Resistivity | 1.00e+8 ohm-cm | 1.00e+8 ohm-cm | IEC 60093 |
BASF Ultramid® B3G8 BK00564 40% Glass Filled PA6 (Conditioned) Ultramid B3G8 BK00564 is a 40% glass filled, pigmented black, injection molding PA6 grade. |
|||
Volume Resistivity | 1.00e+8 ohm-cm @Temperature 140 °C |
1.00e+8 ohm-cm @Temperature 284 °F |
IEC 60093 |
BASF Ultramid® KR 4355 G7 35% Glass Filled PA6/6T (Conditioned) Description: 35% glass-fiber reinforced product for injection-molding; high toughness, strength and stiffness, low water absorption, high melting point (295°C [563°F]). The mechanical properties r.. |
|||
Volume Resistivity | 1.00e+8 ohm-cm | 1.00e+8 ohm-cm | dry; IEC 60093 |
EMS-Grivory Grivory® TSC-10/4 EC black 9832 PA666-CF Information provided by EMS Grivory |
|||
Volume Resistivity | 1.00e+8 ohm-cm | 1.00e+8 ohm-cm | conditioned; IEC 60093 |
EMS-Grivory Grivory® TSC-10/4 EC black 9832 PA666-CF Information provided by EMS Grivory |
|||
Volume Resistivity | 1.00e+8 ohm-cm | 1.00e+8 ohm-cm | |
3M Novec™ 7000 Engineered Fluid 3M™ Novec™ 7000 Fluid unique properties make it useful as a low temperature, heat transfer fluid for cooling reactors in pharmaceutical & chemical processing. It's also ideal for low temperature a.. |