Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 0.0018 ohm-cm | 0.0018 ohm-cm | |
SGL Carbon Group SIGRAFIL C® C10 M250 UNS Milled Carbon Fiber, Unsized Carbon Fiber Milled SIGRAFIL C is excellent for making materials electrically conductive such as powders, dry mixtures, adhesives, floorings, aqueous adhesive systems and all aqueous mixing processes. Milled SIG.. |
|||
Volume Resistivity | 0.0018 ohm-cm | 0.0018 ohm-cm | |
SGL Carbon Group SIGRAFIL C® C10 S003 GLY Staple Carbon Fiber, Glycerine Sizing In its precision cut staple form SIGRAFIL C is a superior free-flowing material suitable for low and high temperature thermoplastic injection-molding processes. It is also an excellent way of making.. |
|||
Volume Resistivity | 0.0018 ohm-cm | 0.0018 ohm-cm | |
SGL Carbon Group SIGRAFIL C® C10 S006 GLY Staple Carbon Fiber, Glycerine Sizing In its precision cut staple form SIGRAFIL C is a superior free-flowing material suitable for low and high temperature thermoplastic injection-molding processes. It is also an excellent way of making.. |