Electrical Properties | Metric | English | Comments |
---|---|---|---|
Volume Resistivity | 0.00030 ohm-cm | 0.00030 ohm-cm | cured 60 minutes at 125°C |
Resin Technology Group TIGA 901 Room Temperature Curing Silver Conductive Epoxy 100 parts resin to 6 parts hardener. Cure 24 hours at 25°C, 1-4 hours at 65°C, 30-60 minutes at 125°C, or 30 minutes at 150°C.TIGA 901 is an electrically conductive, silver filled epoxy adhesiv.. |
|||
Volume Resistivity | 0.00030 ohm-cm | 0.00030 ohm-cm | cured 30 minutes at 150°C |
Resin Technology Group TIGA 908 Gold Bonder - Low Stress Silver Conductive 100 parts resin to 6 parts hardener.TIGA 908 is a low stress, conductive silver filled epoxy adhesive. It is recommended for bonding, and sealing electronic applications which require bonding to gol.. |
|||
Volume Resistivity | 0.00030 ohm-cm | 0.00030 ohm-cm | |
Gwent Electronic Materials C2010903D2 Curable Silver Range This product is based on a unique curing process that results in the low temperature formation of a thermosetting conductive adhesive that combines good adhesion with excellent electrical properties.. |
|||
Volume Resistivity | 0.00030 ohm-cm | 0.00030 ohm-cm | |
Tra-Con Tra-Bond 293-14 Electrically Conductive Silver-Filled Epoxy Adhesive TRA-BOND 293-14 silver-filled, electrically conductive epoxy adhesive is designed to provide strong bonds to difficult-to-bond metals, such as nickel, copper, gold and solder. The stress-absorbing c.. |
|||
Volume Resistivity | 0.00030 ohm-cm | 0.00030 ohm-cm | cured 10 min @ 100°C |
Tra-Con Tra-Duct 2907 Silver-Filled Epoxy Adhesive TRA-DUCT 2907 is an electrically conducting silver-filled medium viscosity epoxy compound recommended for electronic bonding and sealing applications that require a combination of good mechanical an.. |
|||
Volume Resistivity | 0.00030 ohm-cm | 0.00030 ohm-cm | cured 5 min @ 125°C |
Tra-Con Tra-Duct 2958 Snap Cure Conductive Silver Epoxy Adhesive TRA-DUCT 2958 is a two-part, smooth paste of specially refined and processed epoxy and silver components, recommended for electronic, microelectronic and die-attach bonding and sealing applications .. |
|||
Volume Resistivity | 0.00030 ohm-cm | 0.00030 ohm-cm | |
Tra-Con Tra-Duct 2979 Microelectronic Conductive Epoxy Adhesive TRA-DUCT 2979 is a fast curing one-part epoxy adhesive with superior electrical conductivity and bonding capability. It has been shown to retain these properties through hundreds of hours of rapid t.. |
|||
Volume Resistivity | 0.00030 ohm-cm | 0.00030 ohm-cm | |
Tra-Con Tra-Duct 2979LV Microelectronic Conductive Epoxy Adhesive TRA-DUCT 2979LV is a fast curing one-part epoxy adhesive with superior electrical conductivity and bonding capability. It has been shown to retain these properties through hundreds of hours of rapid.. |
|||
Volume Resistivity | 0.00030 ohm-cm @Temperature 150 °C |
0.00030 ohm-cm @Temperature 302 °F |
|
Tra-Con Tra-Duct 8205 One-Part Electrically Conductive Silver-Filled Epoxy TRA-DUCT 8205 is an electrically conducting silver-filled epoxy compound recommended for electronic bonding and sealing applications that require a combination of excellent mechanical and electrical.. |
|||
Volume Resistivity | 0.00030 ohm-cm | 0.00030 ohm-cm | cured 5 min @ 160°C |
Tra-Con Tra-Duct 2902 Room Temperature Conductive Silver Epoxy Adhesive TRA-DUCT 2902 is an electrically conducting silver-filled epoxy compound recommended for electronic bonding and sealing applications that require a combination of good mechanical and electrical prop.. |
|||
Volume Resistivity | >= 0.00030 ohm-cm | >= 0.00030 ohm-cm | |
Epoxy Technology EPO-TEK® E2036 Epoxy Product Description: A two component, slightly flexible, silver-filled, electrically conductive adhesive for semiconductor and electronic assemblies. It is a low Tg epoxy, intended for many kinds o.. |
|||
Volume Resistivity | <= 0.00030 ohm-cm | <= 0.00030 ohm-cm | cured |
Atom Adhesives AA-DUCT 2924 Epoxy Adhesive AA-DUCT 2924 is a two part electrically conductive composition developed for low shrinkage; low resistivity bonding applications where good electrical and physical properties over a wide temperature.. |
|||
Volume Resistivity | 0.00030 ohm-cm | 0.00030 ohm-cm | cured |
Atom Adhesives AA-DUCT 2979 Epoxy Adhesive AA-DUCT 2979 is a fast curing one part epoxy adhesive with superior electrical conductivity and bonding capability. AA-DUCT 2979 has been shown to retain their properties through hundreds of hours o.. |
|||
Volume Resistivity | 0.00030 ohm-cm | 0.00030 ohm-cm | cured 1 hr @ 65°C |
Tra-Con Tra-Duct 2921 Silver-Filled Adhesive Information provided by Tra-Con Inc. |
|||
Volume Resistivity | 0.00030 ohm-cm | 0.00030 ohm-cm | Cured: 1 hour at 60°C |
Resinlab® SEC1233 Silver Filled Epoxy Adhesive Resinlab™ SEC1233 is a silver filled, two component, room temperature curing epoxy adhesive. It is designed to cure completely at room temperature. SEC1233 provides excellent electrical conductivit.. |