Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 15.0 - 38.0 kV/mm | 380 - 965 kV/in | Average value: 25.8 kV/mm Grade Count:12 |
Overview of materials for Polycarbonate, Optical Grade This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Optical Grade". Each property range of values reported is minimum and maximum values of a.. |
|||
Dielectric Strength | 17.0 - 38.0 kV/mm | 432 - 965 kV/in | Average value: 22.2 kV/mm Grade Count:38 |
Overview of materials for Polycarbonate, Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum a.. |
|||
Dielectric Strength | 27.1 - 38.0 kV/mm | 688 - 965 kV/in | Average value: 33.3 kV/mm Grade Count:9 |
Overview of materials for Polycarbonate/ASA Alloy, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ASA Alloy, Unreinforced". Each property range of values reported is minimum and maximum va.. |
|||
Dielectric Strength | 15.0 - 38.0 kV/mm | 381 - 965 kV/in | Average value: 26.6 kV/mm Grade Count:13 |
Overview of materials for Nylon 612, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Unreinforced". Each property range of values reported is minimum and maximum values of approp.. |
|||
Dielectric Strength | 18.7 - 38.0 kV/mm | 475 - 965 kV/in | Average value: 25.5 kV/mm Grade Count:33 |
Overview of materials for Nylon 612, Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Glass Fiber Filler". Each property range of values reported is minimum and maximum values of .. |
|||
Dielectric Strength | 18.0 - 38.0 kV/mm | 457 - 965 kV/in | Average value: 29.9 kV/mm Grade Count:5 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Plating Grade This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Plating Grade". Each property range of values reported is minimum.. |
|||
Dielectric Strength | 8.00 - 38.0 kV/mm | 203 - 965 kV/in | Average value: 23.8 kV/mm Grade Count:27 |
Overview of materials for PBT + PET Blend, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "PBT + PET Blend, Glass Filled". Each property range of values reported is minimum and maximum values of .. |
|||
Dielectric Strength | 16.2 - 38.0 kV/mm | 411 - 965 kV/in | Average value: 21.8 kV/mm Grade Count:25 |
Overview of materials for Polyethylene Terephthalate (PET), Glass/Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Glass/Mineral Reinforced". Each property range of values reported is m.. |
|||
Dielectric Strength | 17.7 - 38.0 kV/mm | 450 - 965 kV/in | Average value: 33.4 kV/mm Grade Count:10 |
Overview of materials for Polytrimethylene Terephthalate (PTT) This property data is a summary of similar materials in the MatWeb database for the category "Polytrimethylene Terephthalate (PTT)". Each property range of values reported is minimum and maximum val.. |