Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 100 - 350 kV/mm | 2540 - 8890 kV/in | Thickness up to 1 µm |
BACT Dylyn® Diamond-Like Nanocomposite Coating a-C:H/a-Si:O nanocomposite. This coating provides the lowest friction of the BACT products, even in high humidity or wet environments. It offers an excellent combination of anti-stick and wear be.. |