Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 16.0 - 19.0 kV/mm @Thickness 0.100 mm |
406 - 483 kV/in @Thickness 0.00394 in |
short term; ASTM D149 |
Polikim EFALON® C-15 PTFE, 15% Glass Filled C15 and C25 have less thermal expansion, higher wear resistance and less deformation under load compared to virgin Efalon® (PTFE). Applications: Seals, Seal rings, gaskets, valve sets, piston rings.. |
|||
Dielectric Strength | 13.0 - 19.0 kV/mm | 330 - 483 kV/in | ASTM D149 |
Polimersan Plastics POLITEF® (PTFE) with 25% Carbon As a result of Filled-In POLITEF® alloys, apart from all of its superior properties, POLITEF®, according to its usage areas has gained additional properties as described below:Electrical Conductiv.. |
|||
Dielectric Strength | 13.0 - 19.0 kV/mm | 330 - 483 kV/in | ASTM D149 |
Polimersan Plastics POLITEF® (PTFE) with 25% Carbon As a result of Filled-In POLITEF® alloys, apart from all of its superior properties, POLITEF®, according to its usage areas has gained additional properties as described below:Electrical Conductiv.. |
|||
Dielectric Strength | 14.0 - 19.0 kV/mm | 356 - 483 kV/in | Average value: 15.7 kV/mm Grade Count:10 |
Overview of materials for Polyaryletherketone (PAEK), Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyaryletherketone (PAEK), Glass Fiber Filled". Each property range of values reported is minimum and m.. |
|||
Dielectric Strength | 16.0 - 19.0 kV/mm | 406 - 483 kV/in | ASTM D149 |
Polimersan Plastics POLITEF® (PTFE) with 15% Glass As a result of Filled-In POLITEF® alloys, apart from all of its superior properties, POLITEF®, according to its usage areas has gained additional properties as described below:Electrical Conductiv.. |
|||
Dielectric Strength | 16.0 - 19.0 kV/mm | 406 - 483 kV/in | ASTM D149 |
Polimersan Plastics POLITEF® (PTFE) with 15% Glass As a result of Filled-In POLITEF® alloys, apart from all of its superior properties, POLITEF®, according to its usage areas has gained additional properties as described below:Electrical Conductiv.. |
|||
Dielectric Strength | 16.9 - 19.0 kV/mm | 430 - 483 kV/in | Average value: 17.8 kV/mm Grade Count:7 |
Overview of materials for Polysulfone, 10% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone, 10% Glass Fiber Reinforced". Specific grades with glass content between 5% and 14% are incl.. |