Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 13.0 - 120 kV/mm | 330 - 3050 kV/in | Average value: 25.5 kV/mm Grade Count:20 |
Overview of materials for Nylon 66/6 This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6". Each property range of values reported is minimum and maximum values of appropriate MatWeb .. |
|||
Dielectric Strength | 11.8 - 120 kV/mm | 300 - 3050 kV/in | Average value: 34.3 kV/mm Grade Count:109 |
Overview of materials for Nylon 66, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Unreinforced". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Dielectric Strength | 9.84 - 120 kV/mm | 250 - 3050 kV/in | Average value: 31.2 kV/mm Grade Count:101 |
Overview of materials for Nylon 66, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Impact Grade". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Dielectric Strength | 15.7 - 120 kV/mm | 400 - 3050 kV/in | Average value: 23.4 kV/mm Grade Count:200 |
Overview of materials for Nylon 66, Heat Stabilized This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Heat Stabilized". Each property range of values reported is minimum and maximum values of appr.. |
|||
Dielectric Strength | 13.8 - 120 kV/mm | 350 - 3050 kV/in | Average value: 50.9 kV/mm Grade Count:6 |
Overview of materials for Nylon 66, MoS2 Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, MoS2 Filled". Each property range of values reported is minimum and maximum values of appropri.. |