Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 30.3 - 98.0 kV/mm | 770 - 2490 kV/in | Average value: 65.2 kV/mm Grade Count:4 |
Overview of materials for PVC, Flexible Grade This property data is a summary of similar materials in the MatWeb database for the category "PVC, Flexible Grade". Each property range of values reported is minimum and maximum values of appropriat.. |