Electrical Properties Metric English Comments
Dielectric Strength 7.00 - 9.00 kV/mm

@Temperature 90.0 °C
178 - 229 kV/in

@Temperature 194 °F
IS 2584-1963
Amity Thermosets ATS 1612 Phenolic Molding Nylon, inorganic, and glass Filler, Compression Molded
Characteristics:High dielectric & mechanical strengthWeather resistant Good electric insulationLow water absorption Good mechanical tension bearing capacityColor-blackSoft/Medium flow Applications:R..
Dielectric Strength 7.00 - 9.00 kV/mm

@Temperature 90.0 °C
178 - 229 kV/in

@Temperature 194 °F
IS 2584-1963
Amity Thermosets ATS 1613-R Phenolic Molding Nylon and glass Filler, Compression Molded
Characteristics:High dielectric & mechanical strengthWeather resistant Good electric insulationLow water absorption Good mechanical tension bearing capacityColor-blackMedium flow Applications:Railwa..
Dielectric Strength 7.00 - 9.00 kV/mm

@Temperature 90.0 °C
178 - 229 kV/in

@Temperature 194 °F
IS 2584-1963
Amity Thermosets ATS 1613-G Phenolic Molding Nylon and inorganic Filler, Compression Molded
Characteristics:High dielectric & mechanical strengthWeather resistant Good electric insulationLow water absorption Good mechanical tension bearing capacityColor-blackSoft/Medium flow Applications:R..