Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 7.00 - 48.0 kV/mm | 178 - 1220 kV/in | Average value: 28.9 kV/mm Grade Count:34 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded". Each property range of values reported is .. |
|||
Dielectric Strength | 11.8 - 48.2 kV/mm | 300 - 1220 kV/in | Average value: 17.0 kV/mm Grade Count:103 |
Overview of materials for Epoxy Encapsulant, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Encapsulant, Unreinforced". Each property range of values reported is minimum and maximum values o.. |