Electrical Properties Metric English Comments
Dielectric Strength 16.7 - 46.0 kV/mm
425 - 1170 kV/in
Average value: 23.3 kV/mm Grade Count:5
Overview of materials for Polysulfone, 20% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are inc..