Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 30.0 - 40.0 kV/mm | 762 - 1020 kV/in | IEC 60243-1 |
Raschig Group AMPLA® 2000 melamine-modified polyester Halogen-free, organically and inorganically filled melamine-modified Polyester molding compound. Low post-shrinkage, very good electrical values, high heat resistance, very good sliding behavior, ve.. |
|||
Dielectric Strength | 30.0 - 40.0 kV/mm | 762 - 1020 kV/in | IEC 60250 |
Raschig Group AMPLA® 7250 melamine-modified polyester Cellulose reinforced melamine-modified Polyester molding compound. Very good electrical values, excellent heat resistance, excellent surface quality, low post shrinkage. This product meets the allow.. |
|||
Dielectric Strength | 12.2 - 40.0 kV/mm | 310 - 1020 kV/in | Average value: 16.1 kV/mm Grade Count:34 |
Overview of materials for Diallyl Phthalate (DAP) Molding Compound, Short Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Diallyl Phthalate (DAP) Molding Compound, Short Glass Fiber Filled". Each property range of values repor.. |
|||
Dielectric Strength | 27.0 - 40.0 kV/mm | 686 - 1020 kV/in | Average value: 31.3 kV/mm Grade Count:11 |
Overview of materials for Polycarbonate/ABS Alloy, Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Glass Fiber Filled". Each property range of values reported is minimum and maxi.. |
|||
Dielectric Strength | 25.6 - 40.0 kV/mm | 650 - 1020 kV/in | Average value: 33.3 kV/mm Grade Count:6 |
Overview of materials for Liquid Crystal Polymer (LCP), 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 20% Glass Fiber Filled". Specific grades with glass content between 15% an.. |
|||
Dielectric Strength | 20.0 - 40.0 kV/mm @Temperature 100 - 200 °C |
508 - 1020 kV/in @Temperature 212 - 392 °F |
Average value: 27.6 kV/mm Grade Count:3 |
Overview of materials for Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled". Specific grades with glass content between 45% an.. |
|||
Dielectric Strength | 20.0 - 40.0 kV/mm @Thickness 0.800 - 3.20 mm |
508 - 1020 kV/in @Thickness 0.0315 - 0.126 in |
Average value: 27.6 kV/mm Grade Count:3 |
Overview of materials for Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 50% Glass Fiber Filled". Specific grades with glass content between 45% an.. |
|||
Dielectric Strength | 25.0 - 40.0 kV/mm | 635 - 1020 kV/in | Average value: 31.6 kV/mm Grade Count:10 |
Overview of materials for Nylon 66/6, 20% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are incl.. |
|||
Dielectric Strength | 18.9 - 40.0 kV/mm | 480 - 1020 kV/in | Average value: 25.7 kV/mm Grade Count:5 |
Overview of materials for Nylon 66/6, 60% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 60% Glass Fiber Reinforced". Specific grades with glass content between 55% and 64% are incl.. |
|||
Dielectric Strength | 20.0 - 40.0 kV/mm @Thickness 2.00 mm |
508 - 1020 kV/in @Thickness 0.0787 in |
IEC 60243 |
Manifattura Cattaneo PVC U Polyvinyl Chloride Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a. |
|||
Dielectric Strength | 20.0 - 40.0 kV/mm | 508 - 1020 kV/in | VDE 0303 |
GEHR Plastics Corzan® PVC-C Polyvinylchloride Polyvinyl chloride is a flame retardant material with an exceptional chemical resistance and also with lower stress cracking. PVC-U shows high mechanical strength, tensile strength and the continuou.. |
|||
Dielectric Strength | 20.0 - 40.0 kV/mm | 508 - 1020 kV/in | ASTM D149/15 |
Mikro-Technik Reproflon PTFE Reproflon is reclaimed PTFE scraps. The powder can be reused for the usual manufacturing procedures.Information provided by Mikro-Technik GmbH |
|||
Dielectric Strength | 30.0 - 40.0 kV/mm | 762 - 1020 kV/in | ASTM D149 |
Guarniflon MFA Fluoropolymer It’s a semi-crystalline fully-fluorinated melt processable fluoropolymer which offer the highest temperature rating and broadest chemical resistance of all melt processable fluoropolymers. It .. |
|||
Dielectric Strength | 30.0 - 40.0 kV/mm | 762 - 1020 kV/in | ASTM D149 |
Guarniflon PFA Perfluoroalkoxy Polymer Fluorinated thermoplastic material, offers the advantages of being thermo-processed whilst at the same time having the properties of PTFE, with excellent chemical and mechanical resistance for appli.. |
|||
Dielectric Strength | 35.0 - 40.0 kV/mm @Thickness 1.00 mm |
889 - 1020 kV/in @Thickness 0.0394 in |
ASTM D149 |
Solvay Specialty Polymers Hyflon® MFA® F1520 Perfluoropolymer Hyflon® F is a family of MFA polymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, high flexural endurance, inherent flame resistance, low s.. |
|||
Dielectric Strength | 35.0 - 40.0 kV/mm | 889 - 1020 kV/in | ASTM D149 |
Solvay Specialty Polymers Hyflon® PFA 420 Perfluoroalkoxy (PFA) Hyflon® PFA is a family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat resistance.. |
|||
Dielectric Strength | 35.0 - 40.0 kV/mm | 889 - 1020 kV/in | ASTM D149 |
Solvay Specialty Polymers Hyflon® PFA M620 Perfluoroalkoxy (PFA) Hyflon® PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat res.. |
|||
Dielectric Strength | 35.0 - 40.0 kV/mm | 889 - 1020 kV/in | ASTM D149 |
Solvay Specialty Polymers Hyflon® PFA M640 Perfluoroalkoxy (PFA) Hyflon® PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat res.. |
|||
Dielectric Strength | 35.0 - 40.0 kV/mm | 889 - 1020 kV/in | ASTM D149 |
Solvay Specialty Polymers Hyflon® PFA P450 Perfluoroalkoxy (PFA) Hyflon® PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat res.. |
|||
Dielectric Strength | 35.0 - 40.0 kV/mm | 889 - 1020 kV/in | ASTM D149 |
Solvay Specialty Polymers Hyflon® PFA P455 Perfluoroalkoxy (PFA) Hyflon® PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat res.. |
|||
Dielectric Strength | 25.0 - 40.0 kV/mm | 635 - 1020 kV/in | ASTM D149 |
Adamas Adalon® 433 PTFE, 10% Ekonol® Information provided by Adamas, HPM |
|||
Dielectric Strength | 35.0 - 40.0 kV/mm | 889 - 1020 kV/in | ASTM D149 |
Solvay Specialty Polymers Hyflon® PFA 420 Perfluoroalkoxy (PFA)
(Unverified Data**) Hyflon® PFA is a family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat resistance, .. |
|||
Dielectric Strength | 35.0 - 40.0 kV/mm | 889 - 1020 kV/in | ASTM D149 |
Solvay Specialty Polymers Hyflon® PFA M620 Perfluoroalkoxy (PFA)
(Unverified Data**) Hyflon PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat resista.. |
|||
Dielectric Strength | 35.0 - 40.0 kV/mm | 889 - 1020 kV/in | ASTM D149 |
Solvay Specialty Polymers Hyflon® PFA M640 Perfluoroalkoxy (PFA)
(Unverified Data**) Hyflon PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat resista.. |
|||
Dielectric Strength | 35.0 - 40.0 kV/mm | 889 - 1020 kV/in | ASTM D149 |
Solvay Specialty Polymers Hyflon® PFA P450 Perfluoroalkoxy (PFA)
(Unverified Data**) Hyflon PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat resista.. |
|||
Dielectric Strength | 16.5 - 40.0 kV/mm | 420 - 1020 kV/in | Average value: 27.6 kV/mm Grade Count:6 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend, Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend, Glass Reinforced". Each property range of values repo.. |
|||
Dielectric Strength | 35.0 - 40.0 kV/mm | 889 - 1020 kV/in | IEC 60243-1 |
Raschig Group 5567 DAP Diallyl Phthalate (DAP), Cast, Mineral Filler Glass-fiber reinforced diallyl phthalate molding compound free from halogens. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exc.. |
|||
Dielectric Strength | 20.0 - 40.0 kV/mm | 508 - 1020 kV/in | VDE 0303 |
GEHR Plastics PVC-U Polyvinylchloride Polyvinyl chloride is a flame retardant material with an exceptional chemical resistance and also with lower stress cracking. PVC-U shows high mechanical strength, tensile strength and the continuou.. |
|||
Dielectric Strength | 0.984 - 40.0 kV/mm | 25.0 - 1020 kV/in | Average value: 15.1 kV/mm Grade Count:41 |
Overview of materials for Epoxy, Molded, Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Molded, Glass Fiber Filler". Each property range of values reported is minimum and maximum values.. |
|||
Dielectric Strength | 19.3 - 40.0 kV/mm | 490 - 1020 kV/in | Average value: 25.1 kV/mm Grade Count:28 |
Overview of materials for Polyethylene Terephthalate (PET), 30% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 30% Glass Reinforced". Specific grades with glass content between 25% .. |