Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 11.81 - 39.37 kV/mm | 300.0 - 1000 kV/in | |
Kraton® D1102 (SBS) Linear Block Copolymer (SBS) styrene-butadiene-styrene block polymer. KRATON® Polymers require no premastication or vulcanization. They can be blended with thermoplastic polymers and significantly improve the impact .. |
|||
Dielectric Strength | 11.81 - 39.37 kV/mm | 300.0 - 1000 kV/in | |
Kraton® D1116 (SB)n Branched Copolymer (SB)n - styrene-butadiene multi-arm (branched) copolymer. KRATON® Polymers require no premastication or vulcanization. They can be blended with thermoplastic polymers and significantly improve .. |
|||
Dielectric Strength | 11.81 - 39.37 kV/mm | 300.0 - 1000 kV/in | |
Kraton® D4141 (SBS) Linear Block Copolymer (SBS) styrene-butadiene-styrene block polymer. KRATON® Polymers require no premastication or vulcanization. They can be blended with thermoplastic polymers and significantly improve the impact .. |
|||
Dielectric Strength | 11.81 - 39.37 kV/mm | 300.0 - 1000 kV/in | |
Kraton® D1101 (SBS) Linear Block Copolymer (SBS) styrene-butadiene-styrene block polymer. KRATON® Polymers require no premastication or vulcanization. They can be blended with thermoplastic polymers and significantly improve the impact .. |
|||
Dielectric Strength | 11.81 - 39.37 kV/mm | 300.0 - 1000 kV/in | |
Kraton® D1112P (SIS) Linear Block Copolymer (SIS) styrene-isoprene-styrene block polymer. KRATON® Polymers require no premastication or vulcanization. They can be blended with thermoplastic polymers and significantly improve the impact q.. |
|||
Dielectric Strength | 21.7 - 39.4 kV/mm | 550 - 1000 kV/in | Average value: 29.2 kV/mm Grade Count:6 |
Overview of materials for Medium Density Polyethylene (MDPE), Extruded This property data is a summary of similar materials in the MatWeb database for the category "Medium Density Polyethylene (MDPE), Extruded". Each property range of values reported is minimum and max.. |
|||
Dielectric Strength | 21.0 - 39.4 kV/mm | 533 - 1000 kV/in | Average value: 29.0 kV/mm Grade Count:19 |
Overview of materials for PVC, Wire and Cable Grade This property data is a summary of similar materials in the MatWeb database for the category "PVC, Wire and Cable Grade". Each property range of values reported is minimum and maximum values of appr.. |