Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 36.8 kV/mm @Thickness 1.60 mm |
935 kV/in @Thickness 0.0630 in |
in air; ASTM D 149 |
SABIC Innovative Plastics Cycolac® X37 ABS ABS, injection moulding, high heat grade.This data was supplied by SABIC-IP for the Americas region. |