Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 35.0 kV/mm | 890 kV/in | 2.03 mm; ASTM D149 |
ExxonMobil Santoprene® 203-50 Thermoplastic Elastomer A hard, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra.. |
|||
Dielectric Strength | 35.0 kV/mm | 890 kV/in | ASTM D149 |
ExxonMobil Santoprene® 211-87 Thermoplastic Elastomer
(discontinued **) A hard, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra.. |
|||
Dielectric Strength | 35.0 kV/mm | 890 kV/in | Arlon-SQA-TMS-020 |
Arlon 44278R018 0.018" Uncured/Cured/Uncured Silicone Rubber Laminate with Fiberglass Substrate Design/Construction:Interleave 1: LDPESide 1 Layer 2: Uncured Silicone RubberSide 1 Layer 1: Cured Silicone RubberSubstrate: Style 1165 FiberglassSide 2: Uncured Silicone RubberInterleave: LDPEUL.. |