Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 34.0 kV/mm | 864 kV/in | |
Ineos ABS Lustran® QE 1120, Extrusion Grade
(discontinued **) General purpose extrusion grade.Information provided by Bayer.LANXESS was spun-off from Bayer in early 2005. Business renamed Ineos ABS after INEOS acquires a majority shareholding under a JV with .. |
|||
Dielectric Strength | 34.0 kV/mm | 864 kV/in | IEC 60243 |
Solvay TECHNYL® A 218 V30 BK 34 NG PA66, 30% glass fiber, DRY Description: TECHNYL® A 218 V30 Black 34 NG is a polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding. The product is available in black color.Benefits: This p.. |
|||
Dielectric Strength | 34.0 kV/mm | 864 kV/in | IEC 60243 |
Solvay TECHNYL® A 218 V35 Black 34 NG PA66, 35% glass fiber, DRY Description: TECHNYL® A 218 V35 Black 34 NG is a polyamide 66, reinforced with 35% of glass fiber, heat stabilized, for injection molding. The product is available in black color.Benefits: This p.. |
|||
Dielectric Strength | 34.0 kV/mm | 864 kV/in | K20/P50; IEC 60243-1 |
Styrolution Luran® 388 S SAN Description: Specialty grade with highest mechanical strength and chemical resistance.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS |
|||
Dielectric Strength | 34.0 kV/mm | 864 kV/in | VDE 0303/4 |
Polyram PF300G3 PBT, 15% Glass Fiber 15% Glass-Fiber reinforced PBT for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Dielectric Strength | 34.0 kV/mm | 864 kV/in | IEC 60250 |
Polyram RamSter PF300G8 PBT, 40% Glass Fiber 40% Glass fiber reinforced PBT for injection molding applications.Information provided by Polyram. |
|||
Dielectric Strength | 34.0 kV/mm | 864 kV/in | IEC 60250 |
Polyram RamSter PF306G6 PBT, 30% Glass Fiber 30% Glass fiber reinforced, low viscosity PBT for injection molding applications.Information provided by Polyram. |
|||
Dielectric Strength | 34.0 kV/mm @Thickness 1.00 mm |
864 kV/in @Thickness 0.0394 in |
IEC 60243-1 |
Covestro Makrolon® 1952 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Flame retardancy• Me.. |
|||
Dielectric Strength | 34.0 kV/mm @Thickness 1.00 mm |
864 kV/in @Thickness 0.0394 in |
IEC 60243-1 |
Covestro Makrolon® 2405 MAS048 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Low.. |
|||
Dielectric Strength | 34.0 kV/mm @Thickness 1.00 mm |
864 kV/in @Thickness 0.0394 in |
IEC 60243-1 |
Covestro Makrolon® 2405 MAS057 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Low.. |
|||
Dielectric Strength | 34.0 kV/mm @Thickness 1.00 mm |
864 kV/in @Thickness 0.0394 in |
IEC 60243-1 |
Covestro Makrolon® 2407 MAS070 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Low.. |
|||
Dielectric Strength | 34.0 kV/mm | 864 kV/in | IEC 60243-1 |
Covestro Makrolon® 2667 Polycarbonate, Flame Retardant Grade ISO 7391-PC,MFLR,(,,)-18-9Global gradeMVR (300 °C/1.2 kg) 12.5 cm3/10 minChlorine- and bromine-free flame retardantUL 94V-2/1.5 mm and 3.0 mmMedium viscosityUV stabilizedEasy releaseInjection moldi.. |
|||
Dielectric Strength | 34.0 kV/mm @Thickness 1.00 mm |
864 kV/in @Thickness 0.0394 in |
IEC 60243-1 |
Covestro Makrolon® 2800 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Med.. |
|||
Dielectric Strength | 34.0 kV/mm @Thickness 1.00 mm |
864 kV/in @Thickness 0.0394 in |
IEC 60243-1 |
Covestro Makrolon® 2805 MAS152 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Med.. |
|||
Dielectric Strength | 34.0 kV/mm | 864 kV/in | IEC 60243-1 |
Covestro Makrolon® 2806 Polycarbonate ISO 7391-PC,M,(,,)-09-9MVR (300 °C/1.2 kg) 9.5 cm3/10 minFood contact qualityMedium viscosityGood hydrolysis resistanceInjection molding - Melt temperature 280 - 320 °CAvailable in transparenttran.. |
|||
Dielectric Strength | 34.0 kV/mm | 864 kV/in | IEC 60243-1 |
Covestro Makrolon® 2867 Polycarbonate, Flame Retardant Grade ISO 7391-PC,MFLR,(,,)-09-9MVR (300 °C/1.2 kg) 9.5 cm3/10 minChlorine- and bromine-free flame retardantUL 94V-2/1.5 mm and 3.0 mmMedium viscosityUV stabilizedEasy releaseInjection molding - Melt tem.. |
|||
Dielectric Strength | 34.0 kV/mm | 864 kV/in | IEC 60243-1 |
Covestro Makrolon® LTG3123 Polycarbonate PreprocessingMax. Water content |
|||
Dielectric Strength | 34.0 kV/mm | 864 kV/in | dry; IEC 60243-1 |
EMS-Grivory Grivory® HT2V-3X V0 black 9021 PA6T/66-GF30 Product description: Grivory HT2V-3X V0 is a 30% glass-fiber reinforced flame retardant (UL 94 V-0) engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Gr.. |
|||
Dielectric Strength | 34.0 kV/mm | 864 kV/in | dry; IEC 60243-1 |
EMS-Grivory Grivory® TSZ 3 PA666 Product description: Grilon TSZ 3 is a heat stabilized, normal viscosity, high impact modified PA66 + PA6 injection molding grade. Grilon TSZ 3 has the following important properties: Excellent toug.. |
|||
Dielectric Strength | 34.0 kV/mm | 864 kV/in | conditioned; IEC 60243-1 |
EMS-Grivory Grivory® XE 3959 black 9992 PA610 Product description: Grilamid XE 3959 is a high viscosity Polyamide 610 especially suitable for extrusion applications. This PA610 product is to a large extent based on renewable raw materials and i.. |
|||
Dielectric Strength | 34.0 kV/mm | 864 kV/in | IEC 60243-1 |
DuPont Performance Polymers Crastin® HR5330HFS BK591 Polybutylene Terephthalate (PBT)
(Unverified Data**) 30% Glass Reinforced Hydrolysis Resistant Polybutylene Terephthalate Crastin HR5330HFS is a 30% glass fiber reinforced moderately toughened hydrolysis resistant polybutylene terephthalate for inject.. |
|||
Dielectric Strength | 34.0 kV/mm | 864 kV/in | IEC 60243-1 |
Covestro Makrolon® 2456 Polycarbonate ISO 7391-PC,MR,(,,)-18-9Global gradeMVR (300 °C/1.2 kg) 19 cm3/10 minFood contact qualityLow viscosityEasy releaseGood hydrolysis resistanceInjection molding - Melt temperature 280 - 320 °CAvailab.. |
|||
Dielectric Strength | 34.0 kV/mm @Thickness 1.00 mm |
864 kV/in @Thickness 0.0394 in |
IEC 60243-1 |
Covestro Makrolon® ET3227 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Extrusion• High visc.. |
|||
Dielectric Strength | 34.0 kV/mm | 864 kV/in | conditioned; IEC 60243-1 |
EMS-Grivory Grivory® TR 90 NZ PAMACM12-I Product description: Grilamid TR grades are transparent thermoplastic polyamides based on aliphatic and cycloaliphatic blocks. Grilamid TR 90 NZ offers a variety of interesting properties such as: o.. |
|||
Dielectric Strength | 34.0 kV/mm | 864 kV/in | IEC 60243-1 |
BASF Ultraform® N2650 Z2 (LEV) POM Description: Is a POM + PUR, elastomer-modified injection-molding grades with high impact strength for clips, snap and fastening elements, also for components subject to impact stress.Information pr.. |
|||
Dielectric Strength | 34.0 kV/mm | 864 kV/in | VDE 0303/4 |
Polyram RamSter PF391G6 PBT, 30% Glass Fiber 30% glass-fiber reinforced, surface modified PBT for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Dielectric Strength | 34.0 kV/mm | 864 kV/in | |
LG Chemical HF350U ABS, High Flow Feature: Injection Molding, High Flow, Good WeatherabilityApplication: E & E Products (Monitor) )CAS No. 9003-56-9Information provided by LG Chemical |
|||
Dielectric Strength | 34.0 kV/mm | 864 kV/in | |
Arkema Group Orgalloy® RS 6030 Nylon 6 Alloy, 30% Glass Fiber (Conditioned) RS 60 series, rigid polyamide 6 alloy: easy to process, chemical resistance (no known solvents) and low moisture absorption leading to stability of mechanical, electrical and dimensional properties.. |