Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 3.40 kV/mm | 86.4 kV/in | 60 Hz, wet, SS; ASTM D149 |
Sumitomo Bakelite North America RX® 448 Cellulose Reinforced Phenolic Novolac RX448 is a cellulose fiber reinforced phenolic novolac molding compound. This material is recommended for large parts requiring moderate toughness. It is designed to meet the requirements of ASTM D.. |
|||
Dielectric Strength | 3.40 kV/mm | 86.4 kV/in | IEC 60243 |
Solvay TECHNYL® 1011R PA6, DRY Description: Polyamide 6, Unfilled, lubricated, for injection molding. Available in: Asia Pacific Product Applications: TECHNYL® 1011R is used in all sectors of industry, offering an excellent flow.. |