Electrical Properties Metric English Comments
Dielectric Strength 30.3 kV/mm
770 kV/in
Short Term; ASTM D149
Quadrant EPP Duratron® PEI U2300 Extruded 30% Glass Reinforced Polyetherimide (ASTM Product Data Sheet)
Dielectric Strength 30.3 - 98.0 kV/mm
770 - 2490 kV/in
Average value: 65.2 kV/mm Grade Count:4
Overview of materials for PVC, Flexible Grade
This property data is a summary of similar materials in the MatWeb database for the category "PVC, Flexible Grade". Each property range of values reported is minimum and maximum values of appropriat..
Dielectric Strength 30.3 kV/mm
770 kV/in
ASTM D149
Westlake Plastics Tempalux® 30% GF Polyetherimide
An amorphous thermoplastic polyetherimide, stock shapes from ULTEM® resin possess a combination of useful characteristics, including high strength at elevated temperatures, high modulus, and broad ..
Dielectric Strength 30.3 kV/mm
770 kV/in
Dow Corning HV 1551/70P
40 Shore hardness low viscosity injection mouldable liquid silicone rubber with high tear strength, high elongation and a fast cure speed.Information provided by Dow Corning
Dielectric Strength 30.3 kV/mm
770 kV/in
AC Rapid Rise; ASTM D149
DuPont™ Nomex® 418 Paper, 3 mil Nominal Thickness
Nomex® Type 418 is designed for high-voltage applications such as motor conductor and coil wrap, transformer ground and layer insulation. It can be readily impregnated with varnishes. This calen..
Dielectric Strength 30.3 kV/mm
770 kV/in
In Air; ASTM D149
Ensinger TECAPEI® 30% Glass Reinforced, made from Ultem® 2300 PEI
TECAPEI™ is an amorphous thermoplastic polyetherimide (PEI) made from Sabic Innovative Plastics' Ultem® 1000 and 2000 series resins. The unreinforced 1000 series materials are translucent amber in..
Dielectric Strength 30.3 kV/mm
770 kV/in
2.03 mm; ASTM D149
ExxonMobil Santoprene® 201-73 Thermoplastic Elastomer
A soft, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra..
Dielectric Strength 30.3 kV/mm
770 kV/in
2.03 mm; ASTM D149
ExxonMobil Santoprene® 211-45 Thermoplastic Elastomer
A soft, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra..
Dielectric Strength 30.3 kV/mm
770 kV/in
ASTM D149
Teknor Apex Fireguard® 910-FOB-NL1 Polyvinyl Chloride, Flexible
Uses: Plenum Cable Jacketing; Wire and Cable Applications Agency Ratings: UL QMTT2 .E200337 Forms: Pellets Additional Information: Dynamic Heat Stability at 205°C, 100 rpm, 72 gr. #5 Bowl (Minutes ..
Dielectric Strength 30.3 kV/mm
770 kV/in
ASTM D149
Quantum PEI - Ultem® 30% Glass Fiber Filled
Information provided by Quantum Advanced Engineering Plastics