Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 27.2 kV/mm | 690 kV/in | in oil; ASTM D149 |
Polymer Resources PEI-G10 Polyetherimide, 10% Glass Reinforced Polyetherimide, 10% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Poly.. |
|||
Dielectric Strength | 27.2 kV/mm | 690 kV/in | ASTM D149 |
Polymer Resources TP-FR-IM Polybutylene Terephthalate, Impact Modified, Flame Retardant, Low Flow Polybutylene Terephthalate, Impact Modified, Flame Retardant, Low FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sa.. |
|||
Dielectric Strength | 27.2 kV/mm | 690 kV/in | ASTM D149 |
Polymer Resources TP-FR-IM-[color]-3 Polybutylene Terephthalate, Impact Modified, Flame Retardant, Low Flow Polybutylene Terephthalate, Impact Modified, Flame Retardant, Low FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sa.. |
|||
Dielectric Strength | 27.2 kV/mm | 690 kV/in | ASTM D149 |
Polymer Resources TPSF-G10 Polybutylene Terephthalate, Structural Foam, 10% Glass Reinforced Polybutylene Terephthalate, Structural Foam, 10% Glass ReinforcedProcess: Foam MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Info.. |
|||
Dielectric Strength | 27.2 kV/mm | 690 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES HiFill FR® PA6/6 FR 144 Availability: North AmericaForms: PelletsAdditive: Lubricant and Heat StabilizerFeatures: Flame Retardant, Halogen Free, Heat Stabilized and LubricatedInformation provided by TP Composites, Inc. |
|||
Dielectric Strength | 27.2 kV/mm | 690 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES HiFill FR® PA6/6 FR 344 Availability: North AmericaForms: PelletsAdditive: Lubricant and Heat StabilizerFeatures: Flame Retardant, Heat Stabilized and LubricatedAppearance: RedInformation provided by TP Composites, Inc. |
|||
Dielectric Strength | 27.2 kV/mm | 690 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES HiFill FR® PA6/6 FR 346 RD Availability: North AmericaForms: PelletsAdditive: Lubricant and Heat StabilizerFeatures: Flame Retardant, Heat Stabilized and LubricatedAppearance: RedInformation provided by TP Composites, Inc. |
|||
Dielectric Strength | 27.2 kV/mm | 690 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES HiFill FR® PA6/6 FR IM HS BK Availability: North AmericaForms: PelletsAdditive: Impact ModifierFeatures: Flame Retardant and Impact ModifiedUL File Number: E157318Appearance: BlackInformation provided by TP Composites, Inc. |
|||
Dielectric Strength | 27.2 kV/mm | 690 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES HiFill FR® PA6/6 FR NAT Availability: North AmericaForms: PelletsFeatures: Flame Retardant UL File Number: E157318Appearance: Natural ColorProcessing Method: Injection MoldingInformation provided by TP Composites, Inc. |
|||
Dielectric Strength | 27.2 kV/mm | 690 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES HiFill FR® PA6 FR 544 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer and LubricantFeatures: Flame Retardant, Lubricated and Heat StabilizedRoHS Compliance: RoHS CompliantInformation provided by TP Com.. |
|||
Dielectric Strength | 27.2 kV/mm | 690 kV/in | |
Dow Corning HV 1520/50 KIT PARTS A&B 50 Shore Hardness injection moldable liquid silicone rubber with high tear strength, high elongation and a fast cure speedInformation provided by Dow Corning |
|||
Dielectric Strength | 27.2 kV/mm | 690 kV/in | 2.03 mm; ASTM D149 |
ExxonMobil Santoprene® 121-73W175 Thermoplastic Elastomer A soft, black, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance, and is designed for .. |
|||
Dielectric Strength | 27.2 kV/mm | 690 kV/in | 2.03 mm; ASTM D149 |
ExxonMobil Santoprene® 101-55 Thermoplastic Elastomer A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range .. |
|||
Dielectric Strength | 27.2 kV/mm | 690 kV/in | ASTM D149 |
3M Scotch-Weld™ DP420 Off-White Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion, and very high levels of durability.Information provided by 3M |
|||
Dielectric Strength | 27.2 kV/mm | 690 kV/in | Arlon SQA-TMS-020 |
Arlon 51271R037 0.037" Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Uncured Silicone RubberInterleave: 2.5 mil PolyethyleneThis data represents typical values for the produ.. |
|||
Dielectric Strength | 27.2 kV/mm | 690 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES HiFill FR® PA6/6 FR HS Availability: North AmericaForms: PelletsAdditive: Lubricant and Heat StabilizerFeatures: Flame Retardant, Heat Stabilized, Halogen Free and LubricatedTPCI# 9857101Information provided by TP Composi.. |
|||
Dielectric Strength | 27.2 kV/mm | 690 kV/in | 2.03 mm; ASTM D149 |
ExxonMobil Santoprene® 111-45 Thermoplastic Elastomer A soft, black, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide range .. |
|||
Dielectric Strength | 27.2 kV/mm | 690 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES HiFill FR® PA6/6 FR 344 BK Availability: North AmericaForms: PelletsAdditive: Lubricant and Heat StabilizerFeatures: Flame Retardant, Heat Stabilized and LubricatedAppearance: BlackInformation provided by TP Composites, Inc. |