Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 27.0 kV/mm | 686 kV/in | ASTM D149/DIN 53481 |
Kolon SPESIN® KP212G30VO G/F Reinforced & Retardant PBT Resin SPESIN® is a thermoplastic PBT resin with excellent thermal, mechanical and electrical properties. SPESIN® is widely used in industrial parts and especially in electrical-electronic parts.High.. |
|||
Dielectric Strength | 27.0 kV/mm @Thickness 1.00 mm |
686 kV/in @Thickness 0.0394 in |
IEC 60243-1 |
Lanxess Pocan® T 7331 POS151 700226 PBT + PET, 30% Glass Fiber PBT + PET, 30% glass fibers, injection molding, improved surface finish, increased temperature peak load, UV stabilizedInformation provided by LANXESS. |
|||
Dielectric Strength | 27.0 kV/mm | 686 kV/in | IEC 60243-1 |
Lanxess Pocan® BF 4409 000000 PBT, 7% Glass Fiber PBT, 7% glass fibers, injection molding, flame retardant |
|||
Dielectric Strength | 27.0 kV/mm | 686 kV/in | IEC 60243 |
Solvay TECHNYL® C 52G1 V20 PA6, Conditioned Description: Halogen and Red Phosphorous free fire resistant polyamide PA6 Glass reinforced for injection molding of thin walled partsAvailable in: Asia Pacific, Europe, Latin America and North Amer.. |
|||
Dielectric Strength | 27.0 kV/mm | 686 kV/in | CEI 93 |
Solvay TECHNYLSTARâ„¢ A205 F Natural S PA6, Eh 0 Description: TECHNYLSTAR A205 F NATURAL S is a polyamide 6.6 with low viscosity for fast cycle molding.Colors: it is supplied in natural color.Available in: Latin America and North AmericaMain Prope.. |
|||
Dielectric Strength | 27.0 kV/mm @Thickness 1.60 mm |
686 kV/in @Thickness 0.0630 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics NORYL NH6020 PPE+HIPS Noryl NH6020 resin is an unfilled, injection moldable modified polyphenylene ether resin. Designed for high heat resistance and thin wall FR performance, this resin delivers a UL94 V0 rating at 0.8 .. |
|||
Dielectric Strength | 27.0 kV/mm @Thickness 1.60 mm |
686 kV/in @Thickness 0.0630 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics NORYL NH6020 PPE+HIPS (Europe-Africa-Middle East) Noryl* NH6020 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for high heat resistance and thin wall FR performance, this resin delivers a UL94 V0 rating at 0.8 mm an.. |
|||
Dielectric Strength | 27.0 kV/mm | 686 kV/in | IEC 243-1 |
Solvay Technyl® A 205F Nylon 66, EH0 Unreinforced polyamide 66, high fluidity, fast cycling grade, for injection molding.Technyl A 205F offers two main advantages: excellent filling qualities and UL 94 V2 under 0.4 mm. It is particula.. |
|||
Dielectric Strength | 27.0 kV/mm | 686 kV/in | IEC 60243-1 |
DSM Arnite® TZ4 254 S PBT-(GF+MD)25 FR(17) Glass/Mineral Reinforced, Flame Retardant |
|||
Dielectric Strength | 27.0 kV/mm | 686 kV/in | dry; IEC 60243-1 |
DSM Novamid® 1013G15 1 NA PA6-GF15 15% Glass Reinforced, Injection Molding |
|||
Dielectric Strength | 27.0 kV/mm | 686 kV/in | dry; IEC 60243-1 |
DSM Novamid® 1013G45 1 NA PA6-GF45 45% Glass Reinforced, Injection Molding |
|||
Dielectric Strength | 27.0 kV/mm | 686 kV/in | dry; IEC 60243-1 |
DSM Novamid® 1013GH15 1 NA/BK37 PA6-GF15 15% Glass Reinforced, Heat Stabilized, Injection Molding |
|||
Dielectric Strength | 27.0 kV/mm | 686 kV/in | AC rapid rise in oil; ASTM D149 |
DuPont™ Nomex® Type 993, 160 mil Nominal Thickness Medium-Density Aromatic Nylon Pressboard Type 993 is a medium-density pressboard which offers a balance of rigidity and conformability along with outstanding saturability and excellent properties in air and oil. Typical applications includ.. |
|||
Dielectric Strength | 27.0 kV/mm | 686 kV/in | dry; IEC 60243-1 |
EMS-Grivory Grivory® TSG-50/4 FA PA666-GF50 Information provided by EMS Grivory |
|||
Dielectric Strength | 27.0 kV/mm | 686 kV/in | dry; IEC 60243-1 |
EMS-Grivory Grivory® TSGL-60/4 nat PA666-GF60 Product description: Grilon TSGL-60/4 natural is based on a heat stabilized semi-crystalline Polyamide PA66+PA6 and 60% long glass fibers. Grilon TSGL-60/4 natural is characterized by the following .. |
|||
Dielectric Strength | 27.0 kV/mm | 686 kV/in | conditioned; IEC 60243-1 |
EMS-Grivory Grivory® TSM-30 PA666-MD30 Product description: Grilon TSM-30 is a heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 30% mineral. Grilon TSM-30 has the following important properties: Excellent surface.. |
|||
Dielectric Strength | 27.0 kV/mm | 686 kV/in | IEC 60243-1 |
DuPont Performance Polymers Crastin® ST820 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) Unreinforced Polybutylene Terephthalate with Excellent Impact Resistance Crastin ST820 NC010 is an unreinforced Super Tough polybutylene terephthalate resin for injection molding.Information provide.. |
|||
Dielectric Strength | 27.0 kV/mm | 686 kV/in | Conditioned; CEI 60243-1 |
Addiplast Addinyl A2 Nylon 66 Unreinforced, medium viscosityInformation provided by Addiplast. |
|||
Dielectric Strength | 27.0 kV/mm | 686 kV/in | Conditioned; CEI 60243-1 |
Addiplast Addinyl A2 W Nylon 66 High molding rateInformation provided by Addiplast. |
|||
Dielectric Strength | 27.0 kV/mm | 686 kV/in | IEC 60243-1 |
DSM Akulon® K223-TP4 (Dry) Impact Modified Nylon 6 (North America) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Dielectric Strength | 27.0 kV/mm | 686 kV/in | IEC 60243-1 |
DSM Arnite® T06 202 /A PBT Medium Viscosity, Injection Molding |
|||
Dielectric Strength | 27.0 kV/mm | 686 kV/in | |
LG Chemical LI912 ASA Description: Good Weatherability, General PurposeApplication: Mail Box, Sprinkler, Sash Joiner, Toy, Satellite Antenna CoverCAS: 26299-47-8Information provided by LG Chemical |