Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 26.1 kV/mm @Thickness 1.50 mm |
663 kV/in @Thickness 0.0591 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics GELOY CR8510 ASA ASA with outstanding UV exposure performance for both exterior and interior applications. F1 Rated. |