Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 25.0 kV/mm | 635 kV/in | IEC 60243-1:1998-01 |
Nylacast Cast Nylon 6, Glass Filled Information provided by Nylacast Ltd. |
|||
Dielectric Strength | 25.0 kV/mm | 635 kV/in | ISO 50243 |
Polikim KESTLUB® Polyamide 6 + Lubricant Kestlub® is a special type of cast polyamide ideal for bearings. It is produced by adding lubricants to cast polyamide through special processes. It performs extremely well in bearing applications .. |
|||
Dielectric Strength | 25.0 kV/mm | 635 kV/in | |
Permabond 2010 Cyanoacrylate, gap filling PERMABOND 200 is a high viscosity product with good flow control useful in wire tacking applications or bonding components. It is fast setting and suitable for use on plastics, rubber and metals. Cy.. |
|||
Dielectric Strength | 25.0 kV/mm | 635 kV/in | |
Permabond 790 Cyanoacrylate, Surface insensitive PERMABOND® 790 is a low viscosity, surface insensitive adhesive that will rapidly bond substrates with acidic surfaces such as wood and plated surfaces. Plastics, metals, ceramics and elastomers ar.. |
|||
Dielectric Strength | 25.0 kV/mm | 635 kV/in | |
3M Dyneon™ Fluorel™ FC-2121 Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. Excellent processability. Suggested .. |
|||
Dielectric Strength | 25.0 kV/mm | 635 kV/in | |
3M Dyneon™ Fluorel™ FC-2178 Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Non-incorporated cure polymer, 65.9%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, 4% Ca(OH)2, 1.4% Dihydroxy Crosslinker, 0.4% Phosp.. |
|||
Dielectric Strength | 25.0 kV/mm | 635 kV/in | |
Plastcom SLOVASTER® B GB 30 PBT, 30% glass beads FeaturesPBT for injection moulding, chemically reinforced with 30% glass beads. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and bending.. |
|||
Dielectric Strength | 25.0 kV/mm | 635 kV/in | IEC 60243-1 |
Solvay Specialty Polymers Ixef® 1622 Polyarylamide (PARA)
(Unverified Data**) Ixef 1622 is an impact modified, 50% glass-fiber reinforced polyarylamide. which exhibits very high strength and rigidity, outstanding surface gloss, and excellent impact resistance. - Natural: Ixef.. |
|||
Dielectric Strength | 25.0 kV/mm | 635 kV/in | ASTM D145 |
Idemitsu Kosan Xarec® WA 550 SPS, 30% Glass Filled Crystalline Polymer, Glass Filled. Used in Automotive and Industrial applications |
|||
Dielectric Strength | 25.0 kV/mm | 635 kV/in | IEC 60243-1:1998-01 |
Global EPP PA 6C IMPACT Cast Polyamide 6 + Plasticizer Cast nylons are generally accepted as the primary engineering polymer, suitable for virtually any plain bearing application. By varying the conditions of polymerisation the mechanical properties of .. |
|||
Dielectric Strength | 25.0 - 30.0 kV/mm | 635 - 762 kV/in | DIN 53481 |
Isoflon PSU Polysulfone Electrical insulating productsRigidHigh chemical, fire and temperature resistanceInformation provided by Isoflon. |
|||
Dielectric Strength | 25.0 kV/mm | 635 kV/in | ASTM D149 |
Mitsui Arlen™ A315 15% Glass Fiber-Reinforced Modified Nylon 6T (DAM) ARLEN™ is a heat resistant, modified polyamide 6T developed by Mitsui Chemicals, Inc. With a high melting point (320°C) and a rigidity level comparable to super engineering plastics, it poss.. |
|||
Dielectric Strength | 25.0 kV/mm | 635 kV/in | IEC 60243-1:1998-01 |
Global EPP PA 612 Copolymer Cast Polyamide 612 Cast nylons are generally accepted as the primary engineering polymer, suitable for virtually any plain bearing application. By varying the conditions of polymerisation the mechanical properties of .. |
|||
Dielectric Strength | 25.0 kV/mm | 635 kV/in | ASTM D149 |
Unitika AX-1500W Conditioned Characteristics: A resin succeeding the advantages of AX1500 resin and containing titanium oxide at high concentration. Improved drastically in light reflection and blocking properties, aimed at dis.. |
|||
Dielectric Strength | 25.0 kV/mm | 635 kV/in | VDE 0303/4 |
Polyram RamSter PF340S6 PBT, 30% Glass Beads 30% Glass beads reinforced PBT for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Dielectric Strength | 25.0 kV/mm @Thickness 2.00 mm |
635 kV/in @Thickness 0.0787 in |
ASTM D149 |
Toyobo Vylopet® EMC430 PET/PBT Blend Key Feature: HB UL-94 ClassApplications: general and high rigidity componentsPET/PBT blends suggested for glossy surfaces. General features of Vylopet® include heat resistance, good mechanical pro.. |
|||
Dielectric Strength | 25.0 kV/mm | 635 kV/in | IEC 60243-1 |
DSM Akulon® K224-G0 (Cond.) 50% Glass Reinforced Nylon 6 (North America) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Dielectric Strength | 25.0 kV/mm | 635 kV/in | IEC 60243-1 |
DSM Akulon® K224-HG7 (Cond.) 35% Glass Reinforced Nylon 6 (North America) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Dielectric Strength | 25.0 kV/mm | 635 kV/in | IEC 60243-1 |
DSM Akulon® S227-C Nylon 66 (European Grade) (Dry) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Dielectric Strength | 25.0 kV/mm | 635 kV/in | No thickness given; ASTM D877 |
ConocoPhillips Synterra™ 1 Hydraulic Oil, AGMA No. 1 Description: Conoco Synterra Environmental Fluids Hydraulic and Circulating Oils give outstanding protection to equipment and the environment. These oils are made from synthetic polyol ester fluids .. |
|||
Dielectric Strength | 25.0 kV/mm | 635 kV/in | IEC 60243 |
Azoty Tarnow™ TARNOFORM 300 GF3 POM 15% glass fiber reinforced injection molding grade, suitable for applications where increased strength and stiffness is required.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A... |
|||
Dielectric Strength | 25.0 kV/mm | 635 kV/in | IEC 60243 |
Azoty Tarnow™ TARNOFORM 700 POM Easy flowing grade for injection molding of thin-walled parts or in case of long flow path.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Dielectric Strength | 25.0 - 30.0 kV/mm | 635 - 762 kV/in | ASTM D149 |
Adamas Adalon® 413 PTFE, 20% PPS Information provided by Adamas, HPM |
|||
Dielectric Strength | 25.0 kV/mm | 635 kV/in | cond; IEC 60243-1 |
DSM Stanyl® TS200F6 PA46-GF30 30% Glass Reinforced |
|||
Dielectric Strength | 25.0 kV/mm | 635 kV/in | IEC 60243 |
Solvay TECHNYL® A 218 PA66, 33% glass fiber, DRY Standard viscosity, heat stabilized for injection molding. It is available in natural and black colors.Benefits: This product offers all the primary properties of unreinforced polyamide 66. In addit.. |