Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 24.3 kV/mm | 618 kV/in | Arlon SQA-TMS-020 |
Arlon T3020-B004 0.020" Self-Fusing, Cured Silicone Rubber Tape with Fiberglass Substrate 1.0 inch wide, 20 mil thick, black, rectangular cross-section, self-fusing silicone tape.Design/Construction:Side 1: Cured Silicone RubberSubstrate: 25% Sinusoidal FiberglassSide 2: Cured Silicone.. |
|||
Dielectric Strength | 24.3 kV/mm | 618 kV/in | Tape Property; ASTM D149 |
Arlon T3030-R004 0.030" (0.762 mm) Thick, 1" wide, Cured Fusible Silicone Rubber with Sinusoidal Fiberglass Substrate Design/Construction: Side 1: Cured Fusible Silicone RubberSubstrate: 25% Sinusoidal FiberglassSide 2: Cured Fusible Silicone Rubber Interleave: Polyester FilmArlon MOX-Tape® Fiberglass Reinforced T.. |