Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 24.0 kV/mm | 610 kV/in | |
Plastcom SLOVALEN PC 16 FRD 1 PP, flame retardant Packaging, transport, stockingThe product is packed in hermetically closed thick-walled 25 kg PE bags, on a 1.000 kg palette coated in a stretch foil, in big bags with a thick PE foil fixed on a 1.0.. |
|||
Dielectric Strength | 24.0 kV/mm | 610 kV/in | STN IEC 60243 |
Plastcom SLOVALEN PC 78 FRD 1 Polypropylene Copolymer, Halogen Flame Retardant, UV Stabilized FeaturesModified copolymer PP with the possibility of changing the MFI within the interval 5 - 20 g/10min. Stabilized against the UV-radiation by the UV stabilizer on the HALS basis. Retarded with.. |
|||
Dielectric Strength | 24.0 kV/mm | 610 kV/in | STN IEC 60243 |
Plastcom SLOVALEN PH 56 FRD 1 Polypropylene Homopolymer, Halogen Flame Retardant FeaturesModified homopolymer PP for injection moulding with increased flammability resistance. Contains flame retardant on the halogen basis. Used in the electrical industry - terminals, coil form.. |
|||
Dielectric Strength | 24.0 kV/mm @Thickness 2.00 mm |
610 kV/in @Thickness 0.0787 in |
ASTM D149 |
Manifattura Cattaneo PEEK Polyetheretherketone Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a. |
|||
Dielectric Strength | 24.0 kV/mm @Thickness 1.00 mm |
610 kV/in @Thickness 0.0394 in |
ASTM D149 |
LG Chemical LUCEL N145LD POM, Chemical Resistance Feature: Injection Molding, POM, Chemical ResistanceApplication: Electric/Electronic Gears, Automobile speaker HousingCAS No. 66455-31-0Information provided by LG Chemical |
|||
Dielectric Strength | 24.0 kV/mm | 610 kV/in | IEC 60243-1 |
Menzolit Menzolit® SMC 0200 Unsaturated Polyester UP SMC 0200 is a general purpose SMC for a wide range of applications. Typically, it is used as housings, covers and functional components in mechanical engineering. The flammability meets the demands .. |
|||
Dielectric Strength | 24.0 kV/mm | 610 kV/in | IEC 60243-1 |
Menzolit Menzolit® SMC 0390 Unsaturated Polyester UP SMC 0390 is a standard low profile SMC. Because of its low shrinkage, the material shows good surface quality as well as very low warpage. The product is suitable for applications if a better surfac.. |
|||
Dielectric Strength | 24.0 kV/mm | 610 kV/in | IEC 60243-1 |
Menzolit Menzolit® SMC 0900 Unsaturated Polyester UP SMC 0900 is a special SMC for use within a chemical aggressive environment. The glass level is selected to combine good mouldability with good strength and stiffness properties. The product is espec.. |
|||
Dielectric Strength | 24.0 kV/mm | 610 kV/in | IEC 60243-1 |
Menzolit Menzolit® SMC 1600 Unsaturated Polyester UP SMC 1600 is a special SMC for sanitary applications. The glass level has been selected to combine good mouldability with good strength and stiffness properties. The material shows an increased resis.. |
|||
Dielectric Strength | 24.0 kV/mm | 610 kV/in | IEC 60243-1 |
Menzolit Menzolit® SMC 0300 Unsaturated Polyester UP SMC 0300 is a low shrink standard SMC providing improved surface quality, reduced shrinkage and warpage. Typical fields of applications are mechanical engineering and electrical industry, where impr.. |
|||
Dielectric Strength | 24.0 kV/mm | 610 kV/in | IEC 60243-1 |
Menzolit Menzolit® SMC 1800 Unsaturated Polyester UP SMC 1800 is for structural applications requiring extreme high mechanical properties and low weight. These compounds mould to parts focussing on mechanical strength for replacement of metals in ord.. |
|||
Dielectric Strength | 24.0 kV/mm | 610 kV/in | IEC 60243-1 |
Solvay Specialty Polymers Ixef® 1032 Polyarylamide (PARA), 60% Glass Fiber (Dry) Ixef® 1032 is a 60% glass-fiber reinforced, general purpose polyarylamide compound which exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance.Featur.. |
|||
Dielectric Strength | 24.0 kV/mm | 610 kV/in | ASTM D149 |
Solvay Specialty Polymers Ryton® QA200N Polyphenylene Sulfide (PPS) Ryton® QA200N (granular powder) unfilled polyphenylene sulfide exhibits excellent thermal stability and chemical resistance.Features: Good Chemical Resistance; Good Thermal StabilityAdditional Pr.. |
|||
Dielectric Strength | 24.0 kV/mm | 610 kV/in | ASTM D149-93 |
Saint-Gobain Pharmed® Biocompatible Tubing for Peristaltic Pumps and Cell Culture Features/Benefits:Outlasts silicone tubing in peristaltic pumps by up to 30 timesLow particulate spallationCan be autoclaved repeatedlyTemperature resistant from -60°F to 275°FWithstands repea.. |
|||
Dielectric Strength | 24.0 kV/mm | 610 kV/in | ASTM D149 |
Samyang Tripet® 2500G30 Polyethylene Terephthalate, 30% Glass Fiber Reinforced TRIPET® has excellent heat resistance, good surface, chemical resistance and high electrical performance.Applications:Coil BobbinConnectorMotor HousingLamp HousingRelay BaseIron bodyAll informati.. |
|||
Dielectric Strength | 24.0 kV/mm @Thickness 1.60 mm |
610 kV/in @Thickness 0.0630 in |
in oil; ASTM D149 |
SABIC Innovative Plastics ULTEM HU2410 PEI (Asia Pacific) 40% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP.. |
|||
Dielectric Strength | 24.0 kV/mm | 610 kV/in | VDE 0303/4 |
Polyram RamLloy PBB701 PC/ABS alloy, UV Stabilized UV stabilized PC/ABS alloy for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Dielectric Strength | 24.0 kV/mm | 610 kV/in | IEC 60243-1 |
Polyplastics Duranex® 3405 Polybutylene Terephthalate (PBT), Standard, 45% GF filled DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Dielectric Strength | 24.0 kV/mm | 610 kV/in | |
Covestro Bayblend® T 65 MN Polycarbonate/ABS Blend High impact and notched impact strength, little risk of brittle fracture, high dimensional accuracy.Applications: Interior automotive components.Information provided by Bayer.As of 1 September 2015,.. |
|||
Dielectric Strength | 24.0 kV/mm | 610 kV/in | dry; IEC 60243-1 |
EMS-Grivory Grivory® TSGK-30 X PA666-(GF+GB)30 Product description: Grilon TSGK-30 X is a heat stabilized PA66 + PA6 injection molding grade with a 30% reinforcement combination (glass fibers and glass beads). Grilon TSGK-30 X has the following .. |
|||
Dielectric Strength | 24.0 kV/mm | 610 kV/in | conditioned; IEC 60243-1 |
EMS-Grivory Grivory® TSGL-40/4 nat PA666-GF40 Product description: Grilon TSGL-40/4 natural is based on a heat stabilized semi-crystalline Polyamide PA66+PA6 and 40% long glass fibers. Grilon TSGL-40/4 natural is characterized by the following .. |
|||
Dielectric Strength | 24.0 kV/mm | 610 kV/in | Arlon SQA-TMS-020 |
Arlon 930-10Rxx-P1 0.030" Self-Fusing Silicone Rubber Tape 1 inch wide, 30 mil thick, red, rectangular cross-section, silicone self-fusing tape. Product is supplied in various yard long roll lengths as indicated by the xx characters in the part number.Desi.. |
|||
Dielectric Strength | 24.0 kV/mm @Thickness 1.00 mm |
610 kV/in @Thickness 0.0394 in |
IEC 60243 |
Ascend Performance Materials Vydyne® 47 NT Nylon 66, Impact Modified, DAM Vydyne® 47 NT is general-purpose, impact-modified PA66 resin. Available in natural, it is recognized for all the processing and property advantages inherent to PA66 with the addition of improved im.. |
|||
Dielectric Strength | 24.0 kV/mm | 610 kV/in | cond.; IEC 243-1 |
Azoty Tarnow™ Tarnamid® T-27 MCS 850 Polyamide 6 - Flame Retarded, Unreinforced Glow wire resistance 850°C, bromine and red phosphorus free, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has .. |
|||
Dielectric Strength | 24.0 kV/mm | 610 kV/in | VDE 0303/4 |
Polyram RamTal PM1013 Acetal, General Purpose General purpose polyacetal copolymer for injection molding applications.Information provided by Polyram Ram On Ind. |
|||
Dielectric Strength | 24.0 kV/mm @Thickness 2.00 mm |
610 kV/in @Thickness 0.0787 in |
IEC 60243-1 |
Victrex® PEEK 450G903 Black Polyetheretherketone, Unreinforced Product Description:High performance thermoplastic material, unreinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding and extrusion, standard flow, FDA food contac.. |