Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 23.7 kV/mm @Thickness 2.00 mm |
602 kV/in @Thickness 0.0787 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics NORYL WCD883 PPE-TPE Flexible and non-halogenated flame retardant extrusion grade intended for evaluation in applications such as jacket of HD 21.14 flexible cables. Flame retardant performance capable of meeting EN 502.. |
|||
Dielectric Strength | 23.7 kV/mm @Thickness 2.00 mm |
602 kV/in @Thickness 0.0787 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics NORYL WCD883 PPE-TPE (Asia Pacific) Flexible and non-halogenated flame retardant extrusion grade intended for evaluation in applications such as jacket of HD 21.14 flexible cables. Flame retardant performance capable of meeting EN 502.. |
|||
Dielectric Strength | 23.7 kV/mm @Thickness 2.00 mm |
602 kV/in @Thickness 0.0787 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics NORYL WCD883 PPE-TPE (Europe-Africa-Middle East) Flexible and non-halogenated flame retardant extrusion grade intended for evaluation in applications such as jacket of HD 21.14 flexible cables. Flame retardant performance capable of meeting EN 502.. |
|||
Dielectric Strength | 23.7 kV/mm | 602 kV/in | |
Covestro Desmopan® 372 Thermoplastic Polyurethane Desmopan 372 is a TPU on the basis of a special ester.Applications: Transport rolls, technical automotive parts.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separa.. |
|||
Dielectric Strength | 23.7 kV/mm | 602 kV/in | |
Covestro Texin® 270 Urethane Thermoplastic Elastomer Key Features:UnfilledSuitable processing methods:Injection moldingInformation provided by Bayer Polymers.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adop.. |