Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 22.8 kV/mm @Thickness 2.00 mm |
579 kV/in @Thickness 0.0787 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics NORYL WCA875 PPE-TPE Non-halogenated flame retardant Flexible Noryl extrusion grade intended for evaluation in applications such as wire insulation and cable jacket. Excellent flame retardant performance with balanced t.. |
|||
Dielectric Strength | 22.8 kV/mm @Thickness 2.00 mm |
579 kV/in @Thickness 0.0787 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics NORYL WCA875 PPE-TPE (Asia Pacific) Non-halogenated flame retardant Flexible Noryl extrusion grade intended for evaluation in applications such as wire insulation and cable jacket. Excellent flame retardant performance with balanced t.. |
|||
Dielectric Strength | 22.8 kV/mm @Thickness 2.00 mm |
579 kV/in @Thickness 0.0787 in |
in oil; IEC 60243-1 |
SABIC Innovative Plastics NORYL WCA875 PPE-TPE (Europe-Africa-Middle East) Non-halogenated flame retardant Flexible Noryl extrusion grade intended for evaluation in applications such as wire insulation and cable jacket. Excellent flame retardant performance with balanced t.. |