Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 22.1 kV/mm @Thickness 1.60 mm |
561 kV/in @Thickness 0.0630 in |
in oil; ASTM D149 |
SABIC Innovative Plastics NORYL GTX APS130 PPE+PPS (Asia Pacific) PPE+PPS GF30% |
|||
Dielectric Strength | 22.1 kV/mm @Thickness 1.60 mm |
561 kV/in @Thickness 0.0630 in |
in oil; ASTM D149 |
SABIC Innovative Plastics NORYL APS130 PPE+PPS (Asia Pacific) |