Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 20.0 kV/mm | 508 kV/in | STN IEC 60243 |
Plastcom SLOVAMID 6 GF 30 LS Polyamide 6, 30% Glass Fiber, UV Stabilization FeaturesPA 6 for injection moulding, chemically reinforced with 30% glass fiber, stabilized against UV-radiation. Used for the grips of electric tools, hobby tools, gears, covers of electric tools... |
|||
Dielectric Strength | 20.0 - 25.0 kV/mm @Thickness 1.00 mm, Temperature 23.0 °C |
508 - 635 kV/in @Thickness 0.0394 in, Temperature 73.4 °F |
ASTM D149 |
Solvay Specialty Polymers Solef® 6010 Polyvinylidene Fluoride (PVDF)
(Unverified Data**) Solef® 6010 PVDF homopolymer has medium viscosity and is typically processed by extrusion.Information provided by Solvay Specialty Polymers. |
|||
Dielectric Strength | 20.0 - 25.0 kV/mm @Thickness 1.00 mm, Temperature 23.0 °C |
508 - 635 kV/in @Thickness 0.0394 in, Temperature 73.4 °F |
ASTM D149 |
Solvay Specialty Polymers Solef® 6012 Polyvinylidene Fluoride (PVDF)
(Unverified Data**) Solef® 6012 PVDF homopolymer is a high-viscosity PVDF resin and is typically processed by extrusion or compression molding.Information provided by Solvay Specialty Polymers. |
|||
Dielectric Strength | 20.0 kV/mm | 508 kV/in | 60°C for 1,000 hrs with 90% RH; JIS-K-6249 |
Fujipoly Industries Sarcon® GR-Hb Gap Filler Pad Sarcon GR-b is a highly conformable, thermally conductive material in areas where space between surfaces is uneven and surface textures vary.Information provided by Fujipoly Industries |
|||
Dielectric Strength | 20.0 kV/mm @Thickness 1.00 mm |
508 kV/in @Thickness 0.0394 in |
ASTM D149 |
LG Chemical LUMID GP2130A(W) PA6+GF13%, General Purpose Feature: Injection Molding, PA6+GF13%, General PurposeApplication: Automotive PartsCAS No. 25038-54-4 and 65997-17-3Information provided by LG Chemical |
|||
Dielectric Strength | 20.0 kV/mm @Thickness 1.00 mm |
508 kV/in @Thickness 0.0394 in |
ASTM D149 |
LG Chemical LUMID GP3300B(W) PA66+MF30%, General Purpose Feature: Injection Molding, PA66+MF30%, General PurposeApplication: Automotive (Engine Cover))CAS No. 25038-54-4 and 9010-79-1Information provided by LG Chemical |
|||
Dielectric Strength | 20.0 kV/mm | 508 kV/in | ASTM D149 |
Kotec Carbotex K-20 Polycarbonate, General Purpose Features: Standard, High flow, TransparentApplications: OA equipment, Communications, Precision parts, Machineries, Safety products, E & E parts, Household applications, Leisure articlesInformation .. |
|||
Dielectric Strength | >= 20.0 kV/mm @Frequency 50.0 Hz |
>= 508 kV/in @Frequency 50.0 Hz |
ASTM D149 |
Iran Petrochemical (PCC) PC 0104 Polycarbonate Suitable for extrusionInformation provided by Iran Petrochemical Commercial Co. |
|||
Dielectric Strength | 20.0 kV/mm | 508 kV/in | Perpendicular (ASTM D149), Short Time |
Haysite 54500 Polyester SMC, 35% Glass Reinforced A high strength fiberglass reinforced thermoset polyester compound formulated for injection, compression, or transfer molding. This material exhibits excellent electrical and mechanical properties, .. |
|||
Dielectric Strength | 20.0 kV/mm @Thickness 2.00 mm |
508 kV/in @Thickness 0.0787 in |
ASTM D149 |
Gromax PBT 2000-201D Product Description: PBT unreinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Excellent mechanic an.. |
|||
Dielectric Strength | 20.0 - 65.0 kV/mm | 508 - 1650 kV/in | DIN 53481 |
Isoflon POM C Polyacetal C Good optical propertiesHigh UV resistanceAbsorbs little moistureInformation provided by Isoflon. |
|||
Dielectric Strength | 20.0 kV/mm | 508 kV/in | DIN 53481 |
Schwartz Technical Plastics LAMIGAMID® 319 Cast Polyamide 6, Oil Filled, Conditioned Application: sheaves and wheels without additional bearings, sliding linersInformation provided by Schwartz Technical Plastics GmbH |
|||
Dielectric Strength | 20.0 kV/mm | 508 kV/in | ASTM D149 |
Samyang Tribit® 1500GN15 Polybutylene Terephthalate, 15% Glass Reinforced, Flame Retardant Characteristics:G/F reinforcedFlame retardantHeat and Impact resistantApplications:AutomotiveConnectorGearOutdoor handleIgnition systemElectronicConnectorGas valveCoil bobbinSwitch caseRelay caseO/A.. |
|||
Dielectric Strength | 20.0 kV/mm | 508 kV/in | IEC 60243-1 |
Polyplastics FR-PET® CN9030 Glass Fiber Reinforced Polyethylene Terephthalate (GF-PET), Flame retardant, General purpose Information provided by PolyPlastics. |
|||
Dielectric Strength | 20.0 kV/mm | 508 kV/in | D149 |
Zhejiang Juner 302-G30 30% Glass Fibre Reinforced, Flammable Resistant, and Low Separate Out Mode Applications: Electrons and Electricity: TV Components, Plugs of Computers, Exhaust Fans of Computers, Plugs, Sockets, Shells of Electronics, Framework of Level Output Transformers, Pipe Pedestals, .. |
|||
Dielectric Strength | 20.0 kV/mm | 508 kV/in | JIS K2111 |
Toyobo PELPRENE™ P80C Polyester TPE, High Flexibility, High Melting Point Features: Polyester TPE, High Flexibility, High Melting PointInformation provided by Toyobo. |
|||
Dielectric Strength | 20.0 kV/mm | 508 kV/in | IEC 60243-1 |
DSM Stanyl® TE250F9 (COND) Nylon 46 45% Glass Reinforced, Heat Stabilized, Flame Retardant (North America) Information provided by DSM Engineering Plastics. |
|||
Dielectric Strength | 20.0 kV/mm | 508 kV/in | Breakdown; DIN 53 481, IEC-243, VDE 0303 Part 1 |
Hippe PEEK Polyetheretherketone PEEK is a crystalline, easily machinable thermoplastic which is characterized by high tensile and constant good electrical properties between 0°-220°C, as well as due to favorable tribological beh.. |
|||
Dielectric Strength | 20.0 kV/mm @Thickness 3.20 mm |
508 kV/in @Thickness 0.126 in |
in oil; IEC 60243-1 |
Eurostar Staramide BG7H PA6, 35% Glass Fiber Filled, Heat Stabilized, Injection Molded Staramide BG7H is a Heat Stabilized, 35% Glass Fiber Reinforced, Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
Dielectric Strength | >= 20.0 kV/mm | >= 508 kV/in | |
China-Yixing Longly Refractories Steatite Ceramics (High Frequency Porcelain) LONGLY's steatite ceramics (namely high frequency porcelain, strengthened porcelain, magnesia porcelain), molecular formula as MgO-SiO2, is pure white. Steatite is the appropriate option when good .. |
|||
Dielectric Strength | 20.0 kV/mm @Thickness 3.20 mm |
508 kV/in @Thickness 0.126 in |
in oil; IEC 60243-1 |
Eurostar Staramide BG3 PA6, 15% Glass Filled, Injection Molded BG3 is a 15% Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Dielectric Strength | 20.0 - 70.0 kV/mm | 508 - 1780 kV/in | ASTM D149 |
Adamas Adalon® 991 PTFE Information provided by Adamas, HPM |
|||
Dielectric Strength | 20.0 kV/mm @Thickness 2.00 mm |
508 kV/in @Thickness 0.0787 in |
ASTM D149 |
Chang Chun Plastic PBT1100L General Purpose PBT Information provided by Dowell Trading Company Ltd. |
|||
Dielectric Strength | 20.0 kV/mm @Thickness 2.00 mm |
508 kV/in @Thickness 0.0787 in |
ASTM D149 |
Beijing Chemical Industry KAIFA® 101 PBT Resin Unreinforced, good toughnessInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Dielectric Strength | 20.0 kV/mm @Thickness 2.00 mm |
508 kV/in @Thickness 0.0787 in |
ASTM D149 |
Beijing Ranger Chem PBT-201-G30 272 Flame Retarding FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Dielectric Strength | 20.0 - 35.0 kV/mm | 508 - 889 kV/in | Average value: 26.0 kV/mm Grade Count:40 |
Overview of materials for Nylon 46, Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Glass Fiber Reinforced". Each property range of values reported is minimum and maximum values .. |
|||
Dielectric Strength | 20.0 kV/mm | 508 kV/in | IEC 672-1 |
CeramTec Rubalit® A 1896 Alumina Rubalit® A 1896 (96%) is an aluminum oxide ceramic with an optimum price/performance ratio. Its outstanding properties are low density, low weight, high corrosion and wear resistance, excellent ele.. |
|||
Dielectric Strength | 20.0 kV/mm @Thickness 3.20 mm |
508 kV/in @Thickness 0.126 in |
Short Time |
Aardvark Polymers Aardalloy® 3326 POM Alloy Rotational Molding Resin Aardalloy 3326 is an acetal alloy formulated for enhanced impact resistance and elongation.Aardalloy 3326 maintains the high degree of chemical resistance and low fuel permeation rates of unfilled a.. |
|||
Dielectric Strength | 20.0 kV/mm @Thickness 1.60 mm |
508 kV/in @Thickness 0.0630 in |
ASTM D149 |
Solvay Specialty Polymers Amodel® AS-4133 HN Polyphthalamide (PPA), Dry, 33% Glass Fiber Reinforcement, Heat Stabilizer Amodel AS-4133 HN polyphthalamide (PPA) is a non-lubricated, heat stabilized grade that offers fast cycle times and is hot-water moldable. Typical applications include electrical and electronic comp.. |