Dielectric Strength 16.6 kV/mm
422 kV/in
Short Time; ASTM D149
Plenco 50015 PET, Pellet, Injection Molded, Black  (discontinued **)
PLENCO 50015 is an engineering grade glass reinforced polyethylene terephthalate resin designed for increased flexibility and good physical strength. It is UL recognized and available in white, natu..
Dielectric Strength 16.6 kV/mm

@Temperature 121 °C,
Time 10800 sec
422 kV/in

@Temperature 250 °F,
Time 3.00 hour
0.125 in. thickness; ASTM D149
Garlock BLUE-GARD® 3400 Compressed Aramid Fiber Gasketing, SBR Binder
Aramid fiber, high-temperature fillers, and SBR binder. Often used in low-pressure saturated steam applications.Excellent SealabilityUnique blend of aramid fibers, fillers, and a SBR rubber binder p..
Dielectric Strength 16.6 kV/mm
422 kV/in
Momentive Performance Materials RTV5812 White Adhesive Sealant, Fast Cure Paste
One-part modified alkoxy cure. Modified alkoxy materials cure at room temperature and will outgas a small amount of ammonia and some alcohol during cure. Typical uses: Fast-curing primerless adhes..
Dielectric Strength 16.6 kV/mm
422 kV/in
Momentive Performance Materials RTV5813 Black Adhesive Sealant, Fast Cure Paste
One-part modified alkoxy cure. Modified alkoxy materials cure at room temperature and will outgas a small amount of ammonia and some alcohol during cure. Typical uses: Fast-curing primerless adhes..
Dielectric Strength 16.6 kV/mm
422 kV/in
Momentive Performance Materials RTV5818 Translucent Adhesive Sealant, Fast Cure Paste
One-part modified alkoxy cure. Modified alkoxy materials cure at room temperature and will outgas a small amount of ammonia and some alcohol during cure. Typical uses: Fast-curing primerless adhes..
Dielectric Strength 16.6 kV/mm

@Thickness 3.20 mm
422 kV/in

@Thickness 0.126 in
in oil; ASTM D149
SABIC Innovative Plastics ULTEM STM1600 PEI Copolymer
Siltem 1600 is a flexible copolymer designed for wire and cable applications. It offers a halogen free (according VDE 0472) flame retardant solution that also offers low smoke emission and toxicity...
Dielectric Strength 16.6 kV/mm
422 kV/in
ASTM D149-97a
DSM Somos® ProtoTherm™ 12110 Water-resistant resin for stereolithography, UV Postcure
DescriptionDSM Somos® 12110 is a liquid photopolymer that produces strong, high temperature tolerant, water-resistant parts. Parts created with Somos® 12110 have a cherry-red appearance which tur..
Dielectric Strength 16.6 kV/mm
422 kV/in
Short Time
Bulk Molding Compounds BMC 1423 Wear Resistant, Electrical Grade