Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 16.1 kV/mm | 409 kV/in | Short Time, 500V/sec; ASTM D149 |
Eastman Eastar GN002 Copolyester, Natural
(discontinued **) Eastar GN002 Copolyester is a glycol modified polyethylene terephthalate (PET) with an added mold release. Eastar GN002 copolyester will not crystallize and thus offers wider processing latitude tha.. |
|||
Dielectric Strength | 16.1 kV/mm | 409 kV/in | Short Time; ASTM D149 |
Plenco 50045 PET, Pellet, Injection Molded, Black
(discontinued **) PLENCO 50045 is an engineering grade glass reinforced polyethylene terephthalate resin designed for higher physical strength. It is UL listed and available in white, natural, and black.Information s.. |
|||
Dielectric Strength | 16.1 - 35.0 kV/mm | 409 - 889 kV/in | Average value: 25.6 kV/mm Grade Count:6 |
Overview of materials for Polycyclohexylenedimethylene Terephthalate (PCT), 30% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "PCT or PCTA, 30% Glass Reinforced".Specific grades with glass content between 25% and 34% are included. .. |
|||
Dielectric Strength | 16.1 kV/mm | 409 kV/in | ASTM D149 |
Wanshijie PETG Sheet PETG is also named GPET. It is made of a kind of non-crystalline PET resin sourced from cyclohexanediol modification. PETG differs greatly from PET and PCT. PETG is a kind of non-crystalline copolym.. |
|||
Dielectric Strength | 16.1 kV/mm | 409 kV/in | Short Time, 500V/sec; ASTM D149 |
Eastman Drystar 0113 Copolyester This product-line is designed to meet the needs of converters seeking value-added solutions to their drying requirements of copolyesters. Eastman’s copolyesters are highly valued for their excellen.. |
|||
Dielectric Strength | 16.1 kV/mm | 409 kV/in | Short Time, 500V/sec; ASTM D149 |
Eastman Spectar® 14471 Copolyester Spectar copolyester extrudes into plastic sheet that is sparkling clear, tough, chemically resistant, odor-free, versatile, easy to work with and affordable. Its toughness allows fabricators to use .. |
|||
Dielectric Strength | 16.1 kV/mm | 409 kV/in | Short Time; ASTM D149 |
Plenco 50130 PET, Pellet, Injection Molded, Black
(discontinued **) PLENCO 50130 is an engineering grade glass reinforced UL flame rated polyethylene terephthalate resin designed for good physical strength. It is UL listed and available in natural and black.Informat.. |
|||
Dielectric Strength | 16.1 kV/mm | 409 kV/in | ST; ASTM D149 |
Sumitomo Bakelite North America FM 4004F Fiberglass and Mineral Reinforced Phenolic Novolac FM 4004F is a fiberglass and mineral reinforced phenolic novolac compound with improved strength properties over FM 4004. This compound exhibits excellent dimensional stability and good strength at.. |