Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | >= 15.7 kV/mm | >= 400 kV/in | Cured |
Resin Technology Group CT-523LV Cationic UV Cure Epoxy Adhesive CT-523-LV is an epoxy-based, low viscosity, cationic-curable adhesive and/or sealant. This product is activated by exposure to medium intensity UV radiation resulting in a high strength, chemical re.. |
|||
Dielectric Strength | >= 15.7 kV/mm | >= 400 kV/in | Cured |
Resin Technology Group CT-988 Cationic UV Cure Epoxy Adhesive CT 988 is an epoxy-based, paste-viscosity, cationic-curable adhesive/sealant. This product is activated by exposure to medium intensity UV radiation resulting in a high strength, chemical resistant,.. |
|||
Dielectric Strength | 15.7 - 155 kV/mm | 400 - 3940 kV/in | Average value: 50.2 kV/mm Grade Count:122 |
Overview of materials for Polystyrene, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Impact Modified". Each property range of values reported is minimum and maximum values of a.. |
|||
Dielectric Strength | 15.7 kV/mm @Thickness 3.17 mm |
400 kV/in @Thickness 0.125 in |
|
Ineos Nova 5730 High flow, High impact
(discontinued **) High flow, High impact, USP Class VIApplications: Toys, Medical, HousewaresProperties were determined on injection molded specimens at 23°C and 50% R.H. unless otherwise specified.Information provi.. |
|||
Dielectric Strength | 15.7 kV/mm | 400 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES HiFill® PA6 GF/M40 L 40% Glass/Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Mineral, 40% Filler by WeightAdditive: LubricantFeatures: LubricatedProcessing Method: Injection MoldingInformation provided by T.. |
|||
Dielectric Strength | 15.7 kV/mm | 400 kV/in | ASTM D 696 |
Styrolution PS 5300 HIPS Excellent ESCRFree of zinc additivesMatte, easily decorated finishGood toughnessUL Classification 94 HBInformation provided by Styrolution |
|||
Dielectric Strength | 15.7 kV/mm | 400 kV/in | ASTM D 696 |
Styrolution PS 5801 HIPS Exceptional processabilityHigh toughnessUSP Class VI certifiedUl Classification 94 HBInformation provided by Styrolution |
|||
Dielectric Strength | 15.7 kV/mm | 400 kV/in | Method A (Short-Time); ASTM D149 |
Techmer ES HiFill® TPU GF40 40% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Dielectric Strength | >= 15.7 kV/mm @Thickness 3.17 mm |
>= 400 kV/in @Thickness 0.125 in |
|
Master Bond EP30ANHT Two Part, Electrically Isolating Epoxy Adhesive Description: Master Bond Polymer System EP30ANHT is a two part epoxy system with terrific thermal conductivity, while maintaining electrical insulation. One noteworthy property is its wide service t.. |
|||
Dielectric Strength | >= 15.7 kV/mm | >= 400 kV/in | Compound Property |
Arlon 10502R010 0.010" (.254 mm) Cured/Post-Cured Unsupported Silicone Rubber Design/Construction:Side 1: Cured/Post-Cured Unsupported Silicone RubberAppearance: Red silicone rubberThis data represents typical values for the production material. The data should not be used to.. |
|||
Dielectric Strength | 15.7 kV/mm | 400 kV/in | ASTM D149 |
Arlon 18609R023 0.023" (0.584 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: PolyethyleneLayer 1: Cured Silicone RubberLayer 2: Uncured Silicone RubberSubstrate: 11523 Style FiberglassThis data represents typical values for the production mate.. |
|||
Dielectric Strength | >= 15.7 kV/mm | >= 400 kV/in | |
Arlon 51589R015 0.015" (0.381 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSide 2: Uncured Silicone RubberThis data Represents typical values for the production material. The data should not be used to write, or in place of,.. |
|||
Dielectric Strength | >= 15.7 kV/mm | >= 400 kV/in | |
Arlon 920-07Rxx-P1 0.020" (0.508 mm) Self-Fusing Silicone Tape Design/Construction:Cross Section Type: RectangularWidth, inches: 0.75Arlon Rectangular Tape: Rectangular tape is of uniform thickness and is ideal for applications where a smooth, even layer of tap.. |
|||
Dielectric Strength | >= 15.7 kV/mm | >= 400 kV/in | |
Arlon R35066R020 0.020" (0.508 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSide 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place of.. |
|||
Dielectric Strength | >= 15.7 kV/mm | >= 400 kV/in | |
Arlon 30580R010 0.010" (0.254 mm) Uncured/Unsupported Silicone Rubber on a Release Carrier Design/Construction:Side 1: Uncured/Unsupported Silicone Rubber on a Release Carrier Appearance: Red silicone gum on polymer linerThis data represents typical values for the production material. The.. |
|||
Dielectric Strength | >= 15.7 kV/mm | >= 400 kV/in | |
Arlon 44571R008A 0.0085" (0.216 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone Rubber Side 2: Uncured Silicone RubberThis data represents typical values for the production material. The data should not be used to write, or in place .. |
|||
Dielectric Strength | >= 15.7 kV/mm | >= 400 kV/in | |
Arlon 51576X015A 0.015" (0.381 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSide 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place of.. |
|||
Dielectric Strength | >= 15.7 kV/mm | >= 400 kV/in | |
Arlon 51970R015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberAppearance: Red gum on glass fiber fabricThis data Represents typical values for the production material. The data should not be used to write, or .. |
|||
Dielectric Strength | >= 15.7 kV/mm | >= 400 kV/in | |
Arlon 56096R025 0.025" (0.635 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone Rubber Side 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place o.. |
|||
Dielectric Strength | >= 15.7 kV/mm | >= 400 kV/in | |
Arlon R31031R025 0.025" Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: 0.003" PolyethyleneSide 1: Uncured Silicone RubberSubstrate: Prime Coated 1564 FiberglassSide 2: Uncured Silicone RubberThis data represents typical values for th.. |
|||
Dielectric Strength | 15.7 kV/mm | 400 kV/in | ASTM D149 |
Arlon R32458R0055E 0.0075" Cured Silicone Rubber with Fiberglass Substrate and Acrylic PSA Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 2113 FiberglassSide 2: Acrylic PSAInterleave: PolypropyleneThis data represents typical values for the production material and sh.. |
|||
Dielectric Strength | 15.7 - 19.7 kV/mm | 400 - 500 kV/in | Average value: 17.7 kV/mm Grade Count:12 |
Overview of materials for Nylon 6, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, PTFE Filled". Each property range of values reported is minimum and maximum values of appropria.. |
|||
Dielectric Strength | >= 15.7 kV/mm | >= 400 kV/in | |
Arlon 44580R010 0.010" (0.254 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberAppearance: Red silicone gum on fiberglass clothThis data represents typical values for the production material. The data should not be used to wri.. |
|||
Dielectric Strength | >= 15.7 kV/mm | >= 400 kV/in | |
Arlon 44686W013 0.013" (0.330 mm) Cured/Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSide 2: Uncured Silicone Rubber UL Recognition: 220°C per UL Card E54153Appearance: White silicone gum on fiberglassThis data represents typical val.. |
|||
Dielectric Strength | 15.7 kV/mm | 400 kV/in | |
Resinlab® EP1285HD-10 Highly Filled, Medium Viscosity Casting Resin Resinlab™ EP1285 (Formerly Lab Product W021901 series) is a highly filled, medium viscosity black casting resin designed for applications requiring a high degree of thermal conductivity and a low C.. |
|||
Dielectric Strength | 15.7 kV/mm | 400 kV/in | ASTM D149 |
Saint-Gobain Meldin® 2001 Bearing General Notes on Meldin 2000 Series Bearing Products:For High-Temperature, Close-Tolerance Applications. Able to withstand temperatures of 600°F with excursions to 900°F, the Medlin 2000 Series ca.. |
|||
Dielectric Strength | >= 15.7 kV/mm | >= 400 kV/in | |
Arlon 47573R007 0.0075" (0.190 mm) Cured Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured RubberSide 2: Cured Rubber This data represents typical values for the production material. The data should not be used to write, or in place of, material specifica.. |