Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 152 kV/mm | 3860 kV/in | ASTM D149 |
Total PSC 1441 Easy Flow, High Heat Resistance Polystyrene Total Petrochemicals Polystyrene 1441 is an easy flowing crystal polystyrene designed for extrusion or injection applications. In extrusion, it improves extruder output and thermoforming cycle time.. |
|||
Dielectric Strength | 152 kV/mm | 3860 kV/in | ASTM D149 |
Total PSC 1050 High Heat Resistance, High Molecular Weight Crystal Polystyrene Total Petrochemicals Polystyrene 1050 is a high heat resistance, high molecular weight crystal polystyrene mainly for the extrusion industry. It is particularly useful in the production of thick sh.. |
|||
Dielectric Strength | 152 kV/mm | 3860 kV/in | ASTM D149 |
Total PSI 2451 High Heat Resistance Impact Polystyrene Total Petrochemicals Polystyrene 2451 is a high heat resistance, impact polystyrene for injection blow molding, thermoforming. It is recommended for the manufacturing of articles which require good.. |