Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 14.8 kV/mm | 376 kV/in | ASTM D149 |
Quadrant EPP Semitron® MP-370 (ASTM Product Data Sheet) |
|||
Dielectric Strength | 14.8 kV/mm | 376 kV/in | Short Time; ASTM D149 |
Plenco 50125 PET, Pellet, Injection Molded, White
(discontinued **) PLENCO 50125 is an engineering grade glass reinforced UL flame rated polyethylene terephthalate resin designed for excellent dimensional stability. It is UL listed and available in white only.Inform.. |
|||
Dielectric Strength | 14.8 kV/mm | 376 kV/in | ASTM D149 |
Plenco 5303 Black Electrical Grade Mineral/Flock Filled Phenolic Molding Compound
(discontinued **) Plaslok 5303 is a two-stage, mineral and flock-filled phenolic molding compound designed for use in appliance, automotive and electrical applications. It can be molded by compression, transfer or i.. |
|||
Dielectric Strength | 14.8 kV/mm | 376 kV/in | Short Time; ASTM D149 |
Sumitomo Bakelite Durez® 29502 Phenolic, Compression Grade Durez 29502 Brown Phenolic is a two stage, asbestos free, glass filled, special purpose molding material. It is formulated for close tolerance applications such as transmission valve bodies, and di.. |
|||
Dielectric Strength | 14.8 kV/mm | 376 kV/in | Short Time; ASTM D149 |
Plenco 1530 Polyester, Briquette, Transfer Molded PLENCO 01530 is a glass and mineral reinforced pelletized polyester molding compound, offering improved mechanical strength properties along with excellent electrical properties and dimensional stab.. |
|||
Dielectric Strength | 14.8 kV/mm | 376 kV/in | |
Covestro Desmopan® 192 Thermoplastic Polyurethane Desmopan 192 is a TPU on the basis of a standard ester.Applications: Castors, coupling elements, seals.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from .. |
|||
Dielectric Strength | 14.8 kV/mm | 376 kV/in | |
Covestro Texin® 950 Urethane Thermoplastic Elastomer Key Features:UnfilledSuitable processing methods:Injection moldingProfile extrusionSheet extrusionInformation provided by Bayer Polymers.As of 1 September 2015, Bayer MaterialScience was separated f.. |
|||
Dielectric Strength | 14.8 kV/mm | 376 kV/in | ASTM D149 |
Plaslok 5303 Black Electrical Grade Mineral/Flock Filled Phenolic Molding Compound
(discontinued **) Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use.Plaslok 5303 is a two-stage, mineral and floc.. |
|||
Dielectric Strength | 14.8 kV/mm | 376 kV/in | ST; ASTM D149 |
Sumitomo Bakelite North America FM 4017F Fiberglass and Mineral Reinforced Phenolic FM 4017F is a fiberglass and mineral reinforced phenolic molding compound, with excellent dimensional stability and good strength at elevated temperatures. Information supplied by Sumitomo Bak North.. |
|||
Dielectric Strength | 14.8 kV/mm | 376 kV/in | 60Hz, Step-by-Step, wet; ASTM D149 |
Sumitomo Bakelite North America FS-10-VO-200-P Short-Glass Reinforced Diallyl Phthalate Short glass fiber reinforced, flame retardant, diallyl meta-phthalate molding compound with excellent heat resistance.Meets the requirements of ASTM D5948 Type SIG-F.Information provided by Vyncolit.. |
|||
Dielectric Strength | 14.8 kV/mm | 376 kV/in | 60Hz, Step-by-Step, wet; ASTM D149 |
Sumitomo Bakelite North America FS-5 Short-Glass Reinforced Diallyl Phthalate Short glass fiber reinforced, non-flame retardant, diallyl meta-phthalate molding compound which meets the requirements of ASTM D5948 TYPE SIG.Information provided by Vyncolit, a Sumitomo Bak Group |