Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 14.6 kV/mm | 370 kV/in | ASTM D149 |
Quantum PPSU Information provided by Quantum Advanced Engineering Plastics |
|||
Dielectric Strength | 14.6 kV/mm | 370 kV/in | ASTM D149 |
ITW Devcon Metal Repair Ceramic Repair Putty, Dark Blue Information provided by ITW Devcon |
|||
Dielectric Strength | 14.6 kV/mm | 370 kV/in | |
Tra-Con Tra-Cast 3109 Low Cost Epoxy Casting System TRA-CAST 3109 is a versatile epoxy casting system developed for solvent-free production casting, potting, encapsulating, and coating applications where low cost, easy handling and flowability, and e.. |
|||
Dielectric Strength | 14.6 kV/mm | 370 kV/in | |
Tra-Con Tra-Bond 2101 General Purpose Epoxy Adhesive TRA-BOND 2101 is a medium viscosity epoxy formulation recommended for laminating, bonding, repair and other adhesive applications where the combination of its superior structural, mechanical and ele.. |
|||
Dielectric Strength | 14.6 kV/mm | 370 kV/in | |
Cytec (Conap) FR-1210 / EA-117 Conapoxy® Resin / Conacure® Hardener Epoxy Potting and Encapsulating Systems for Electronic ApplicationsHigh technology epoxy resin systems for potting and encapsulation, for the defense, aerospace, electronics, computer, automotive an.. |
|||
Dielectric Strength | 14.6 kV/mm | 370 kV/in | ASTM D149 |
Arlon 56609R028 0.029" Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: 3 mil PELayer 2: Uncured Silicone RubberLayer 1: Cured Silicone RubberSubstrate: Style 1564 FiberglassThis data represents typical values for the production materi.. |
|||
Dielectric Strength | 14.6 kV/mm | 370 kV/in | ASTM D1000 |
3M SJ5300 Protective Product, Molded Shapes 3M Bumpon Protective Products Molded Shapes – Colored and Clear Series are pressure-sensitive, adhesive-back polyurethane products. They can be used as feet, stops, spaces, and protectors in many a.. |
|||
Dielectric Strength | 14.6 kV/mm | 370 kV/in | ASTM D1000 |
3M SJ5400 Protective Product, Molded Shapes 3M Bumpon Protective Products Molded Shapes – Colored and Clear Series are pressure-sensitive, adhesive-back polyurethane products. They can be used as feet, stops, spaces, and protectors in many a.. |
|||
Dielectric Strength | 14.6 - 16.5 kV/mm | 370 - 420 kV/in | Short Time |
Bulk Molding Compounds BMC 100 Thermoset Polyester, GP BMC 100 is a high strength, low shrink general purpose molding compound. It can be supplied in bulk or extruded in pre-weighted slugs. Due to the excellent flow and controlled reactivity, BMC 100 is.. |
|||
Dielectric Strength | 14.6 - 15.7 kV/mm | 370 - 400 kV/in | short time |
Bulk Molding Compounds BMC T12-17394 General Purpose Molding Compound BMC T12-17394 is a general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC T12 is well suited for injection, transfer or compression molding of intricate parts. .. |
|||
Dielectric Strength | 14.6 - 16.5 kV/mm | 370 - 420 kV/in | Short Time |
Bulk Molding Compounds BMC 200 Thermoset Polyester, Electrical Grade BMC 200 is a high strength, low shrink molding compound. It can be supplied in bulk or extruded in pre-weighted slugs.Typical applications are circuit breakers, insulators, bobbins, electrical conne.. |
|||
Dielectric Strength | 14.6 - 15.7 kV/mm | 370 - 400 kV/in | Short Time |
Bulk Molding Compounds BMC 5592 Arc, Track, and Weather Resistant Polyester BMC 5592 molding compound is an arc, track and weather resistant grade polyester compound suitable for compression, transfer and stuffer injection molding. It has excellent impact strength, flame re.. |
|||
Dielectric Strength | 14.6 - 15.7 kV/mm | 370 - 400 kV/in | short time |
Bulk Molding Compounds BMC T12(18) General Purpose Molding Compound BMC T12(18) is a general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC T12 is well suited for injection, transfer or compression molding of intricate parts. Ty.. |
|||
Dielectric Strength | 14.6 kV/mm | 370 kV/in | ASTM D149 |
Devcon Fastmeal™ Epoxy Precision Repair EpoxyComments: High-performance, alumina-filled epoxy putty for making fast, dependable emergency repair to leaks in pipes carrying ores, coal, cement, san and gravel. Cures in 5 m.. |
|||
Dielectric Strength | 14.6 - 37.0 kV/mm | 370 - 940 kV/in | Average value: 18.4 kV/mm Grade Count:11 |
Overview of materials for Polyethersulfone (PES), 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone (PES), 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% .. |
|||
Dielectric Strength | 14.6 kV/mm | 370 kV/in | |
Atom Adhesives AA-BOND 2101 Epoxy Adhesive AA-BOND 2101 is a clear medium viscosity epoxy formulation recommended for laminating, bonding, repair and other adhesive applications where the combination of superior structural, mechanical and el.. |