Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 13.2 kV/mm | 335 kV/in | Short Time; ASTM D149 |
Plenco 7300 Phenolic, Nodular, Transfer Molded
(discontinued **) Two-Stage Phenolic. PLENCO 07300 is an organic fiber reinforced phenolic molding compound offering improved mechanical strength and excellent cosmetic properties. UL recognized under component file.. |
|||
Dielectric Strength | 13.2 kV/mm | 335 kV/in | ASTM D149 |
Plenco 5314 Black (COM) Impact Grade Phenolic Molding Compound
(discontinued **) Plaslok 5314 is the replacement material for the former Union Carbide BMMA-5314. It is a two-stage, impact grade phenolic molding compound suitable for compression, transfer or injection molding of.. |
|||
Dielectric Strength | 13.2 kV/mm | 335 kV/in | ASTM D149 |
Plenco 5314 Black (INJ) Impact Grade Phenolic Molding Compound
(discontinued **) Plaslok 5314 is the replacement material for the former Union Carbide BMMA-5314. It is a two-stage, impact grade phenolic molding compound suitable for compression, transfer or injection molding of.. |
|||
Dielectric Strength | 13.2 kV/mm | 335 kV/in | Short Time; ASTM D149 |
Plenco 6582 Phenolic, Briquette, Transfer Molded PLENCO 06582 is a rubber modified phenolic molding compound, offering excellent heat resistant properties, along with improved mechanical strength at elevated temperatures. UL recognized under compo.. |
|||
Dielectric Strength | 13.2 kV/mm | 335 kV/in | Short Time; ASTM D149 |
Plenco 7507 Phenolic, Granular, Compression Molded PLENCO 07507 is an organic reinforced phenolic molding compound offering improved dimensional stability under humid conditions. 07507 offers excellent resistance to degradation from detergent solut.. |
|||
Dielectric Strength | 13.2 kV/mm | 335 kV/in | Short Time; ASTM D149 |
Plenco 4301 Phenolic, Granular, Compression Molded PLENCO 04301 is a heat resistant, mineral filled phenolic molding compound offering excellent dimensional stability and electrical properties. UL recognized under component file E40654. 04301 is ava.. |
|||
Dielectric Strength | 13.2 kV/mm | 335 kV/in | Step by Step; ASTM D149 |
Plenco 4568 Phenolic, Granular, Compression Molded PLENCO 04568 is a heat resistant, mineral and flock filled, phenolic molding compound, formulated to provide thermal oxidation stability along with excellent dimensional stability. 04568 is availabl.. |
|||
Dielectric Strength | 13.2 - 14.2 kV/mm | 335 - 361 kV/in | ASTM D149-97a |
DSM Somos® ProtoGen™ O-XT 18420 Epoxy Resin for Stereolithography, UV Postcure at HOC -2 DescriptionDSM Somos® ProtoGen O-XT 18420 is a liquid, ABS-like, photopolymer that produces accurate parts ideal for general purpose applications. ProtoGen resins are the first SL resins to demons.. |
|||
Dielectric Strength | 13.2 - 15.2 kV/mm | 335 - 385 kV/in | short time |
Bulk Molding Compounds BMC G10(12) Mineral Filled, Glass Fiber Reinforced Polyester BMC G10 is a general purpose, mineral filled, glass fiber-reinforced polyester that is suitable for compression, transfer and stuffer injection molding. G10 is well suited to applications where hig.. |
|||
Dielectric Strength | 13.2 - 15.2 kV/mm | 335 - 385 kV/in | short time |
Bulk Molding Compounds BMC T15(GP) General Purpose Molding Compound BMC T15(GP) is a high strength, low shrink general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC T15(GP) is well suited for a variety of applications. It is av.. |
|||
Dielectric Strength | 13.2 - 15.2 kV/mm | 335 - 385 kV/in | short time |
Bulk Molding Compounds BMC T40(25)-XHS Die Casting Replacement Grade Molding Compound BMC T40(25)-XHS is a high strength molding compound with excellent dimensional stability. It is UL recognized and is available in a wide range of colors. Because of its superior physical propertie.. |
|||
Dielectric Strength | 13.2 - 15.2 kV/mm | 335 - 385 kV/in | short time |
Bulk Molding Compounds BMC T40(25)-XHS-15869 Die Casting Replacement Grade Molding Compound BMC T40(25)-XHS-15869 is a high strength molding compound with excellent dimensional stability. It is UL recognized and is available in a wide range of colors. Because of its superior physical pro.. |
|||
Dielectric Strength | 13.2 - 15.2 kV/mm | 335 - 385 kV/in | short time |
Bulk Molding Compounds BMC T60 Grey Wear Resistant Molding Compound BMC T60 Grey is a wear resistant molding compound specifically formulated for applications that require excellent abrasion resistance. Due to its low specific gravity it has substantial cost per cu.. |
|||
Dielectric Strength | 13.2 - 15.2 kV/mm | 335 - 385 kV/in | short time |
Bulk Molding Compounds BMC T40(18)V0 Die Casting Replacement Grade Molding Compound BMC T40(18)V0 is a lower cost version of BMC T40(18) where a UL 5V rating is not necessary. |
|||
Dielectric Strength | 13.2 kV/mm | 335 kV/in | ASTM D149 |
Plaslok 5314 Black (COM) Impact Grade Phenolic Molding Compound
(discontinued **) Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use.Plaslok 5314 is the replacement material for .. |
|||
Dielectric Strength | 13.2 kV/mm | 335 kV/in | ASTM D149 |
Plaslok 5314 Black (INJ) Impact Grade Phenolic Molding Compound
(discontinued **) Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use.Plaslok 5314 is the replacement material for .. |
|||
Dielectric Strength | 13.2 - 15.2 kV/mm | 335 - 385 kV/in | short time |
Bulk Molding Compounds BMC T40(18) Die Casting Replacement Grade Molding Compound BMC T40(18) was formulated as a direct replacement for aluminum die casting applications. T40(18) is UL recognized. Excellent mechanical properties and dimensional control allow molded parts to ma.. |
|||
Dielectric Strength | 13.2 - 15.2 kV/mm | 335 - 385 kV/in | short time |
Bulk Molding Compounds BMC T40(20) Die Casting Replacement Grade Molding Compound BMC T40(20) was formulated as a direct replacement for aluminum die casting applications. T40(20) is UL recognized. Excellent mechanical properties and dimensional control allow molded parts to ma.. |
|||
Dielectric Strength | 13.2 - 15.2 kV/mm | 335 - 385 kV/in | short time |
Bulk Molding Compounds BMC T40-4020-AQ High Strength Arc Quenching Molding Compound BMC T40-4020-AQ was formulated as a high strength arc quenching material for electrical applications. Typical applications are arc hoods and electrical contactors.Information provided by Bulk Moldi.. |
|||
Dielectric Strength | 13.2 - 15.2 kV/mm | 335 - 385 kV/in | short time |
Bulk Molding Compounds BMC T60-6006 Wear Resistant Molding Compound BMC T60-6006 is a wear resistant molding compound specifically formulated for applications that require excellent abrasion resistance. Due to its low specific gravity it has substantial cost per cu.. |
|||
Dielectric Strength | 13.2 - 15.2 kV/mm | 335 - 385 kV/in | short time |
Bulk Molding Compounds BMC T60-6009 Compression Grade Wear Resistant Molding Compound BMC T60-6009 is a compression grade wear resistant molding compound. This material was specifically formulated for applications that require excellent abrasion resistance. Due to its low specific .. |