Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 12.4 - 130 kV/mm | 315 - 3300 kV/in | Average value: 23.5 kV/mm Grade Count:58 |
Overview of materials for Polysulfone (PSU) This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone". Each property range of values reported is minimum and maximum values of appropriate MatWeb.. |
|||
Dielectric Strength | 12.4 kV/mm | 315 kV/in | ASTM D149 |
Gharda Chemicals Gafone™ T6300 Polysupersulfone (PSS)
(discontinued **) Characteristics: Excellent Dimensional Properties Transparent High Mechanical Properties Good Electrical Properties High Tg of 270°C and expected Continuous Use Temperature of 220°C App.. |
|||
Dielectric Strength | 12.4 kV/mm | 315 kV/in | ASTM D149 |
Gharda Chemicals Gafone™ T6500 Polysupersulfone (PSS)
(discontinued **) Characteristics: Excellent Dimensional Properties Transparent High Mechanical Properties Good Electrical Properties High Tg of 270°C and expected Continuous Use Temperature of 220°C App.. |
|||
Dielectric Strength | 12.4 kV/mm | 315 kV/in | 200°C for 1,000 hrs |
Fujipoly Industries Sarcon® 85H Thin-Film HR Sarcon HR is Fujipolys originally developed High Heat Conductive Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Sarcon GHR is a composite of .. |
|||
Dielectric Strength | 12.4 kV/mm | 315 kV/in | Perpendicular S/T in Air; ASTM D-149 |
Glastic 1130 Angles, Channels, and Structural Shapes Information provided by Glastic Corporation |
|||
Dielectric Strength | 12.4 kV/mm | 315 kV/in | Short Time; ASTM D149 |
Plenco 1501 Polyester, Briquette, Transfer Molded PLENCO 01501 is a general purpose, mineral filled granular polyester molding compound, offering excellent arc and track resistance properties, low post shrinkage, and improved mechanical strength va.. |
|||
Dielectric Strength | 12.4 kV/mm | 315 kV/in | Short Time; ASTM D149 |
Plenco 1501 Polyester, Pellet, Injection Molded PLENCO 01501 is a general purpose, mineral filled granular polyester molding compound, offering excellent arc and track resistance properties, low post shrinkage, and improved mechanical strength va.. |
|||
Dielectric Strength | 12.4 kV/mm | 315 kV/in | Short Time; ASTM D149 |
Plenco 1586 Polyester, Pellet, Transfer Molded PLENCO 01586 is a glass and mineral reinforced pelletized polyester molding compound offering excellent heat resistance and mechanical strength properties. This product is typically used for injecti.. |
|||
Dielectric Strength | 12.4 - 14.6 kV/mm | 315 - 370 kV/in | Short Time |
Bulk Molding Compounds BMC 300 Mineral Filled, Glass Reinforced Polyester BMC 300 is a general purpose, mineral filled, glass fiber-reinforced polyester that is suitable for compression, transfer and stuffer injection molding. Our Granite-X series of molding compounds bel.. |
|||
Dielectric Strength | 12.4 kV/mm @Thickness 3.17 mm |
315 kV/in @Thickness 0.125 in |
Short-Time 500 V/sec |
Solvay Specialty Polymers Hylar® MP20 PVDF Polyvinylidene Fluoride
(discontinued **) Data provided by the manufacturer.Hylar® polymers have the characteristic stability of fluoropolymers combined with a unique polarity that influences its solubility and electrical properties. In a.. |
|||
Dielectric Strength | 12.4 kV/mm | 315 kV/in | Perpendicular S/T in Air; ASTM D-149 |
Glastic GLASGUARD 1130 Corrosion-Resistant Panels GlasGuard Grade 1130 is a fiberglass-reinforced thermoset polymer composite system which is available as sheet stock or in a variety of pultruded shapes. Grade 1130 possesses flame resistance, corr.. |