Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 11.81 - 39.37 kV/mm | 300.0 - 1000 kV/in | |
Kraton® D1102 (SBS) Linear Block Copolymer (SBS) styrene-butadiene-styrene block polymer. KRATON® Polymers require no premastication or vulcanization. They can be blended with thermoplastic polymers and significantly improve the impact .. |
|||
Dielectric Strength | 11.81 - 39.37 kV/mm | 300.0 - 1000 kV/in | |
Kraton® D1116 (SB)n Branched Copolymer (SB)n - styrene-butadiene multi-arm (branched) copolymer. KRATON® Polymers require no premastication or vulcanization. They can be blended with thermoplastic polymers and significantly improve .. |
|||
Dielectric Strength | 11.81 - 39.37 kV/mm | 300.0 - 1000 kV/in | |
Kraton® D4141 (SBS) Linear Block Copolymer (SBS) styrene-butadiene-styrene block polymer. KRATON® Polymers require no premastication or vulcanization. They can be blended with thermoplastic polymers and significantly improve the impact .. |
|||
Dielectric Strength | 11.81 - 39.37 kV/mm | 300.0 - 1000 kV/in | |
Kraton® D1101 (SBS) Linear Block Copolymer (SBS) styrene-butadiene-styrene block polymer. KRATON® Polymers require no premastication or vulcanization. They can be blended with thermoplastic polymers and significantly improve the impact .. |
|||
Dielectric Strength | 11.81 - 39.37 kV/mm | 300.0 - 1000 kV/in | |
Kraton® D1112P (SIS) Linear Block Copolymer (SIS) styrene-isoprene-styrene block polymer. KRATON® Polymers require no premastication or vulcanization. They can be blended with thermoplastic polymers and significantly improve the impact q.. |