Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 1.06 kV/mm | 26.9 kV/in | |
ICHS Fiberfax® Alumina-Silica Ceramic Fibers Fiberfrax® ceramic fibers are made from high-purity alumina-silica materials. ICHS uses Fiberfrax® ceramic fiber to manufacture vacuum-formed products in:High-Temperature DuctworkCombustion C.. |